Nickel Alloy Nimonic 75 UNS N06075

\

Short Introduction:

HY N75/Nimonic 75/UNS N06075/W.Nr. 2.4951/W.Nr. 2.4630/AFNOR NC20T is a nickel-chromium alloy with good mechanical properties and oxidation resistance at high temperatures. Alloy 75 is most commonly used for sheet metal fabrications which require oxidation and scaling resistance together with medium strength at high operating temperatures. Alloy 75 is also used in gas turbine engines, for components of industrial furnaces, for heat treating equipment and fixtures, and in nuclear engineering.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY N75 Material grades and equivalents

    Nimonic 75/ UNS N06075 / W.Nr. 2.4951 / W.Nr. 2.4630 / AFNOR NC20T

     

     

    Chemical Composition 

    Alloy

    %

    C

    Cr

    Ni

    Ti

    Fe

    Cu

    Mn

    Si

    75

    Min.

    0.08

    18

    Balance

    0.2

    Max

    0.15

    21

    0.6

    5

    0.5

    1

    1

     

    HY N75 Physical properties:

    Density

    8.37 g/cm3

    Melting point

    2450-2520℃

     

    HY N75 minimum mechanical properties in the room temperature:

     

    Alloy

    Tensile strength

    Thermal conductivity

    Coefficient of thermal expansion

    HardnessHB

    Rm N/mm2

    W/m• °C

    μm/m/°C

    HY N75(solution)

    1400-2210

    11.7

    11

    241

     

    Alloy 75 (UNS N06075) is a nickel-chromium alloy with good mechanical properties and oxidation resistance at high temperatures. Alloy 75 is most commonly used for sheet metal fabrications which require oxidation and scaling resistance together with medium strength at high operating temperatures. Alloy 75 is also used in gas turbine engines, for components of industrial furnaces, for heat treating equipment and fixtures, and in nuclear engineering.

     

    Specifications

    Rod, Bar, Wire and Forging Stock BS HR 5, BS HR 504, DIN 17752, AECMA PrEN2306, AECMA PrEN2307, AECMA PrEN2306, AECMA Pr EN2307, AECMA PrEN2402, ISO 9723, ISO 9724, ISO 9725
    Plate, Sheet, Strip BS HR 203, DIN 17750, AECMA PrEN2293, AECMA PrEN2302, AECMA PrEN2411, ISO 6208
    Pipe and Tube BS HR 403, DIN 17751, AECMA PrEN2294, ISO 6207
    Other DIN 17742, AECMA PrEN2308, Werkstoff Nr 2.4630, W. Nr 2.4951, UNS N06075, HY N75 (tradename), MSRR 7104 and MSRR 7004, AFNOR NC 20T

     

    Typical Mechanical Properties Alloy 75

    Rupture Strength (1000 h)

    Temperature

    psi

    MPa

    760°C / 1400° F

    6000

    40

    815°C / 1500°F

    3500

    24

    870°C / 1600°F

    2200

    15

    925°C / 1700°F

    1500

    10

    980°C / 1800°F

    1200

    8

    Specification

    Rod, Bar, Wire and Forging Stock

    BS HR 5, BS HR 504, DIN 17752, AECMA PrEN2306, AECMA PrEN2307, AECMA PrEN2306, AECMA Pr EN2307, AECMA PrEN2402, ISO 9723, ISO 9724, ISO 9725, MSRR 7004

    Plate, Sheet, Strip

    BS HR 203, DIN 17750, AECMA PrEN2293, AECMA PrEN2302, AECMA PrEN2411, ISO 6208, MSRR 7104

    Pipe and Tube

    BS HR 403, DIN 17751, AECMA PrEN2294, ISO 6207

    (This material was Annealed)

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy





  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !