Cobalt Alloy Refractaloy 26 UNS R30188

\

Short Introduction:

R26/GB GH26/UNS Refractaloy-26/SEW VDIUV W. Nr.1.2888 has excellent resistance to relaxation, anti creep property, permanence property and resistance to stress corrosion resistance.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY R26 Material grades and equivalents

    R26/GB GH26/UNS Refractaloy-26/SEW VDIUV W. Nr.1.2888

     

    HY R26 Chemical composition

    Alloy

    %

    Ni

    Cr

    Fe

    Mo

    Ti

    Co

    R26

    Min

    Rest

    Max

    37

    18

    3.0

    2.7

    20

     

    HY R26 Characteristic

    HY R26 has excellent resistance to relaxation, anti creep property, permanence property and resistance to stress corrosion resistance.

    Physical properties:

    Density:9.14 g/cm3

    Melting point:1300℃-1330 ℃

    Alloy sheet mechanical properties in the room temperature:

    Alloy Status Tensile strength
    Rm N/mm²
    Yield strengthRP0.2 N/mm² Elongation
    A5 %
    Solution Treatment 925 610 10

     

    HY R26 Application field

    HY R26 is a material can be applied in turbine engine blade and fastener.

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy





  • Previous:
  • Next:

  • Send your message to us:

    INQUIRY NOW
    • * CAPTCHA: Please select the House

    RELATED PRODUCTS

    INQUIRY NOW
    • * CAPTCHA: Please select the Cup