Cobalt Alloy Stellite 6 UNS R3006

\

Short Introduction:

HY S6/Stellit 6/UNS R3006/AMS 5387C-2001 is the most widely used of the wear resistant cobalt-based alloys and exhibits good all-round performance. It is regarded as the industry standard for general-purpose wear resistance applications.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY S6 Material grades and equivalents: Stellit 6; UNS R3006; AMS 5387C-2001

    Introduction:

    HY S6 is the most widely used of the wear resistant cobalt-based alloys and exhibits good all-round performance. It is regarded as the industry standard for general-purpose wear resistance applications.

    HY S6 Chemical components

    C

    Cr

    Si

    W

    Fe

    Mo

    Ni

    Mn

    B

    Co

    1.2

    28

    1.1

    4.5

    3

    3

    1

    bal

    *The chemical composition shown above is an outline only,and should not be taken as a full specification.
    *Note that cored wire may have higher Fe contents than other product forms.

    HY S6 Physical property (Room Temp.)

    Density
    (lb/in³)
    Specific
    Gravity
    Solidus Liquidus Specific heat
    (J/kg·K)
    Magnetic
    Permeability
    Electrode
    Potential
    Electrical
    Conductivity
    Electrical
    Resistivity
    0.305 8.46 2340°F 2540°F 0.101°F
    Btu/lb-
    <1.2@200
    Oersteds
    -0.25
    Volts
    1.9%IACS
    (Int. Annealed Copper Std.)
    41.73
    microhms-inch

    HY S6 Thermal Properties-Conductivity & Expansion

    Thermal Expansion Coefficient Thermal Conductivity by Temperature
    °F Microinch/
    inch-°F
    °C Microns/
    m-°C
    °F Btu/ft2/in/
    hr/°F
    °C W/mk
    212 6.3 100 11.34 70 102.7 21.11 14.82
    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy



  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !
    WhatsApp Online Chat!