Breve introduzione:

HY 926 / Incoloy 926 / Alloy926 / UNS N08926 / W.Nr.1.4529 t har høj modstandsdygtighed over for grubetæring og spaltekorrosion når i halogenid og H2S indeholdt syre media.In praksis, effektiv modstand af klorid spændingskorrosion.


  • Fob pris: US $ 25-80 / Kilogram
  • Min.order mængde: 300 kg
  • Порт: Shanghai
  • Betalingsbetingelser: L / C, T / T, 30% ned betaling efter ordre, balance mod kopi af B / L
  • Dettagli del prodotto

    Tags på produkter

    HY 926 Væsentlige kvaliteter og ækvivalenter

    Incoloy 926 /  Alloy926 / UNS N08926 / W.Nr.1.4529

    HY 926 Kemisk sammensætning:

    Legering

    %

    Ni

    Cr

    Fe

    C

    Миннесота

    си

    Cu

    momento

    N

    Ti

    P

    S

    926

    Min.

    24

    19

    Equilibrio

    0.5

    6.0

    0,15

    0,6

    Max.

    26

    21

    0.02

    2

    0.5

    1.5

    7,0

    0.25

    1.2

    0.03

    0.01

    HY 926 Fysiske egenskaber:

    density

    8,1 g / cm3

    Smeltepunkt

    1320-1390 ℃

    HY 926 Alloy Minimum Mekaniske egenskaber i rumtemperaturen:

    Alloy tilstand

    trækstyrke
    Rm N / mm2

    Udbytte styrke
    RP0.2N / mm2

    forlængelse
    A5%

    926

    650

    295

    35

    HY 926 Karakteristisk:
    1.It has high resistance to pitting and crevice corrosion when in Halide and H2S contained acid media.
    2.In practice, effective in resistance of chloride stress corrosion cracking.
    3.A variety of corrosion have good corrosion resistance capability in the normal oxidation and restore environment.
    4.Upgrade mechanical properties than Cronifer 1925 LC-Alloy 904 L.
    5. Alloys has Improved the stability of metallurgical compared to a range of 18% of the nickel content alloys.
    6.With a certification of applied in manufacturing-related pressure vessel (VdTUV-196~400℃ and ASME )
    metallurgisk struktur
    926 is face-centered cubic lattice structure.
    Rustbeskyttelse
    926 is an austenitic stainless steel alloy has a similar chemical composition with 904L alloy, its nitrogen content is 0.2%, molybdenum content is 6.5%. Molybdenum and nitrogen content significantly increased the resistance of pitting and crevice corrosion in the halide media.Meantime, nickel and nitrogen not only ensures the stability of metallographical, but also reduce separating intergranular trend in the thermal process or welding process better than the nitrogen content of nickel alloy. 926 has particular corrosion resistance in the chloride ions medium due to the excellent local corrosion resistance and 25% nickel alloy content.A variety of experiments in the 10000-70000ppm of Chloride concentration, PH 5-6, 50-68℃ operating temperature of the slurry of limestone FGD system show that, after a 1-2 year trial period, 926 alloy without pitting and crevice corrosion.926 in other chemical media also has good corrosion resistance in the high temperature and high concentration of media, including sulfuric acid, phosphoric acid, acid gas, sea water, salt and organic acids.926 is the material that choosed for BAM directory Chapter 6 of “dangerous goods storage and transportation containers norms” by Berlin, Germany’s national Institute for Materials Research and Testing (BAM) . In addition, in order to have the best corrosion resistance only when the material is in the right state of metallurgy and guarantee clean conditions.
    Application field:
    Alloy 926 is a multipurpose material can be applied in many industrial:
    1. Fire system, water purification system, marine engineering and hydraulic piping perfusion system
    2. The pipeline, joint, air systems in the acidic gas production
    3. Evaporator, the heat exchanger, filter, mixer, etc. in the phosphate production
    4.Power plants condensation and pipe system in the use of sewage water to cool water
    5. The use of acidic organic catalyst chlorinated derivatives production
    6. The production of cellulose pulp bleacher
    7. Polished bar in the orrosive oil wells
    8. Hose system in the ocean engineering
    9. Flue gas desulphurization system components
    10. Sulfuric acid condensation and separation system
    11. Crystalline salt concentration and the evaporator
    12. Transport of corrosive chemicals containers
    13. Reverse osmosis desalination plant

    forma regolare per tutti i tipi di leghe
    Modulo specificazione fornitura Modulo Andre
    Ark Spessore: 0.40-4.75mm, Generale Larghezza: 1000,1219,1500mm Tutta la bobina o di parte di esso Ricotto a freddo, superficiale 2B, 2E
    Plade Spessore: 4.76-60mm, Larghezza: 1500,2000,2500mm, Lunghezza: 3000,6000,8000,8500mm (piastra di base 10 millimetri può essere arrotolato) Tutta la bobina o di parte di esso laminazione a caldo singolo, stato solido soluzione ricotto, 1D Surface
    Bælte Tykkelse: 0.10-3.0mm, Bredde: 50-500mm Tutta la bobina o formato specificato Ricotto a freddo, superficiale 2B, 2E
    Bar & Rod Laminati barΦ5-45mm, Length≤1500mm Lucido Bar (cerchio, quadrato) Soluzione ricottura, decalcificazione
    Forged barΦ26-245mm, Length≤4000mm
    tubo Weld Outer diameterΦ4.76-135mm, Muro Thickness0.25-4.00mm, Lunghezza: ≤35000 mm Base sul vostro requisito
    tubi senza saldatura Outer diameterΦ3-114mm, Muro Thickness0.2-4.5mm Base sul vostro requisito
    Tråd Outer diameterΦ0.1-13mm Base sul vostro requisito Ni Ni & lega, Ti e Ti lega
    forgiato skiver, ringe, pladser, blokke, plader Base sul vostro requisito Acciaio, lega
    Flangs Tutti i tipi di Flangs Base sul vostro requisito Acciaio, lega
    saldatura Materiale filo della bobina Φ0.025mm-1,6 millimetri Base sul vostro requisito Certificato di Origine: America, Svezia, Gran Bretagna, Germania, Austria, Italia, Francia.
    Dritto WireΦ1.6mm-4,0 millimetri
    Saldatura rodΦ1.2mm-4,0 millimetri
    Rør Gomito, tre collegamenti, quattro collegamenti, formato differente diametro Base sul vostro requisito Ni Ni & lega, Ti e Ti lega
    Explosive laminato composito Foglio Thickness≥2mm Raw Base sul vostro requisito Ni Ni & lega, Ti e Ti lega



  • Forrige:
  • Næste:

  • RELATEREDE PRODUKTER

    WhatsApp Online Chat !