Discount wholesale Nickel Alloy Incoloy 925 UNS N09925 for Montreal Factory
Innovation, quality and reliability are the core values of our company. These principles today more than ever form the basis of our success as an internationally active mid-size company for Discount wholesale Nickel Alloy Incoloy 925 UNS N09925 for Montreal Factory, we have built a reliable reputation among many customers. Quality&customer first are always our constant pursuit. We spare no efforts to make better products. Look forward to long-term cooperation and mutual benefits!
Y925 Material grades and equivalents
HY 925 /UNSN09925
HY 925 Chemical compostion:
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
S |
Al |
Ti |
P |
Mo |
HY 925 |
Min. |
42 |
19.5 |
bal |
1.5 |
0.15 |
1.9 |
2.5 |
|||||
Max. |
46 |
23.5 |
0.03 |
1 |
0.5 |
3 |
0.03 |
0.50 |
2.4 |
0.03 |
3.5 |
HY 925 Physical properties:
Density |
8.14 g/cm3 |
Melting point |
1343 ℃ |
HY 925 minimum mechanical properties in the roomtemperature
Alloy state |
Tensile strength |
Yield strength RP0.2 N/mm² |
Elongation A 5 % |
Solution treatment |
650 |
300 |
30 |
HY 925 Characteristic as below :
This is an age-hardenable alloy of nickel-chromium-iron. The additions of titanium and aluminum enable it to be age-hardened while molybdenum and copper contents enhance resistance to corrosive media. Designed primarily for applications in the production of gas.
HY 925 Application field:
It is used in the petroleum industry for applications such as gas well components, valves and tubing, as well as finding use in high-strength piping systems.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Melting down 1 gram bars of Silver, Copper, Nickel and Brass with hydrogen and oxygen. Brass is previously an alloy of copper and zinc, and did not soften down effortless as a I figured out from my Brass, Guide and Gunpowder video clip. I then blend the a few workable metals Silver, copper and nickel to generate…….Silvcopickel
SUBSCRIBE: http://comprehensive.sc/1bnslc9
Facebook: http://comprehensive.sc/1dT2aaM
RHNB Vs. Watermelon – http://comprehensive.sc/1bns60F
RHNB Vs. Jello – http://comprehensive.s/1bns0WF RHNB Vs. Elmers Glue – http://comprehensive.sc/1dT1TEM
RHNB Entire Playlist – http://comprehensive.sc/1dT1WjP -Want to ship an object / materials / substance to be RHNB’d or HHO’d? Send Here with a comprehensive credit of your donation! PO Box 21 96 Seymour St. Tonawanda NY 14150 Usa
Qingdao NPA Marketplace Co. Ltd is a foremost manufacturer specialized in centrifugal casting tube and static castings of warmth resistant alloys, which include ethylene cracking furnace tube, reformer furnace tube, CAL(constant annealing traces) &CGL(constant galvanizing traces) furnace roller and radiant tube, glass lehr roller and warmth/have on resistant castings. The annual potential is 9000 tons centrifugal casting tube and 3500 tons static castings (500 tons precision castings).
Internet site: www.npa-china.com