Hot Sale for Nickel Alloy Inconel 718 UNS N07718 Supply to Swansea
Dedicated to strict quality control and thoughtful customer service, our experienced staff members are always available to discuss your requirements and ensure full customer satisfaction for Hot Sale for Nickel Alloy Inconel 718 UNS N07718 Supply to Swansea, If you are interested in any of our products and services, please don't hesitate to contact us. We are ready to reply you within 24 hours after receipt of your request and to create mutual un-limited benefits and business in near future.
HY 718 Material grades and equivalents
Inconel 718 / GB GH4169 / UNS N07718 / SEW VDIUV W.Nr.2.4668 NiCr19Fe19Nb5Mo3 / BS NA 51 / AFNOR NC19FeNb
HY 718 Chemical composition
Alloy |
% |
Ni |
Cr |
Fe |
Mo |
Nb |
Co |
C |
Mn |
Si |
S |
Cu |
Al |
Ti |
718 |
Min. |
50 |
17 |
balance |
2.8 |
4.75 |
0.2 |
0.7 |
||||||
Max. |
55 |
21 |
3.3 |
5.5 |
1 |
0.08 |
0.35 |
0.35 |
0.01 |
0.3 |
0.8 |
1.15 |
HY 718 Physical properties
Density |
8.2 g/cm³ |
Melting point |
1260-1340 ℃ |
HY 718 Alloy minimum mechanical properties in the roomtemperature
Alloy |
Tensile strength |
Yield strength |
Elongation |
Brinell hardness |
Solution treatment |
965 |
550 |
30 |
≤363 |
718 Characteristic as below:
1.workability
2.High tensile strength,endurance strength,creep strength and rupture strength at 700℃.
3.High inoxidability at1000℃.
4.Steady mechanical performance in the low temperature.
5.Good welding performance.
HY 718 Metallurgical structure
718alloy is Austenitic structure, precipitation hardening generate “γ” made it excellent mechanical performance. G rain boundary generate “δ” made it the best plasticity in the heat treatment.
HY 718 Corrosion resistance
718 alloy with extremely resistance to stress corrosion cracking and pitting ability in high temperature or low temperature environments, especially the inoxidability in the high temperature.
HY 718 Application field:
The elevated temperature strength, excellent corrosion resistance and workability at 700℃ properties made it use in a wide range of high requirement environments.
1.Steam turbine
2.Liquid-fuel rocket
3.Cryogenic engineering
4.Acid environment
5.Nuclear engineering
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China
Inconel 718, The Severe Metal Alloy. http://www.techsteel.web/alloy/nickel/inconel-718
Turbine Blades have revolutionized air vacation and electricity era.
Hundreds of slim precision blades spinning at a hundred,000 RPM have to have a materials that can stand up to excessive disorders.
Inconel 718 is a distinctive metal alloy that can stand up to excessive temperatures from -423° to 1300°F
This alloy is aged hardened, making it possible for it to be welded without having hardening for the duration of heating and cooling.
The improvement of Inconel began in the fifties for use in vital steam line plants. Originally used for armed service programs it was later on adopted by the professional sector.
Inconel 718‘s tolerance for excessive temperature make it specially perfectly suited for programs such as
turbine blades
nuclear electricity plants, and
aerospace programs. It was used in the space shuttles high force pump.
AMS 5589 | AMS 5596 | AMS 5597 | AMS 5663 | AMS 5664
For extra inconel 718 details take a look at techsteel.web
Tech Steel provides Specialty Alloys and Supplies.
Check out www.techsteel.web or phone 1-631-223-7638