Hot sale reasonable price Iron Alloy Precision Alloy 1J50 Factory from Nairobi
We are proud of the high customer satisfaction and wide acceptance due to our persistent pursuit of high quality both on product and service for Hot sale reasonable price Iron Alloy Precision Alloy 1J50 Factory from Nairobi, Let's cooperate hand in hand to jointly make a beautiful future. We sincerely welcome you to visit our company or contact us for cooperation!
HY J50 Material grades and equivalents
1J50 / JIS PB
HY J50 Chemical composition
Grade |
C |
P |
S |
Mn |
Ni |
Si |
Mn |
Cu |
Fe |
||||
≤ |
|||||||||||||
HY J50 |
0.03 |
0.020 |
0.020 |
0.3-0.6 |
49.5-50.5 |
0.15-0.30 |
0.30-0.60 |
≤0.20 |
Rest |
HY J50 Alloy Mechanical properties in the room temperature
Grade |
Shape |
Magnetic properties |
|||
Initial permeabilityμO |
Maximum permeabilityμm |
Hc |
Saturation induction density BS |
||
HY J50 |
Cold rolling strips |
≥3.8 |
≥62.5 |
≤9.6 |
1.5 |
Forging bar |
≥3.1 |
≥31.3 |
≤14.4 |
1.5 |
HY J50 Characteristic as below
The HY J50 has rectangular hysteresis loop and high saturation magnetic induction, is mainly used to worked at a moderate magnetic field magnetic amplifier, choke ring, rectifier circle, as well as the computer device components.
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Riporto(placcatura)con filo Nimonic 80 dia. one.2 eseguito con inverter multiprocesso Weldtronic Synertech 8004 Digit in pulsato sinergico.
NB .Il lampeggio dell’arco è presente solo nella ripresa effettuata dalla fotocamera digitale usata probabilmente a causa di interferenza con l’intenso arco luminoso.
Details: belda1@tiscali.it
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China