Nikel Alloy Nimonic 90 UNS N09901

\

Pendahuluan singkat:

HY N90 / Nimonic 90 / GB GH90 / UNS N07090 / BS Nimonic90 / W. Nr. 2,4632 yang  aging strengthen ni-based deformation high temperature ally, with a high amount of cobalt and many kinds of strengthening element, this alloy in 815 ~ 870 °C have high tensile strength and contravariance ability, good oxidation resistance and corrosion resistance, cold and heat alternately repeatedly in under the action of a higher fatigue strength and good formability and weldability. Used for turbine engine turbine dish, leaf, high temperature fasteners, card hoop, seals and elastic components etc.

 


  • Harga fob: US $ 25 - 80 / Kilogram
  • Min.order kuantitas: 300kg
  • Port: Shanghai
  • Istilah Pembayaran: L / C, T / T, 30% uang muka setelah pesanan, keseimbangan terhadap salinan B / L
  • Rincian produk

    Tags produk

    HY N90  nilai Material dan setara

    Nimonic 90 / GB GH90 / UNS N07090  /BS  Nimonic90/ W. Nr. 2,4632

    HY N90 karakteristik dan bidang aplikasi Ringkasan:

    paduan ini adalah penuaan memperkuat sekutu deformasi suhu tinggi berbasis ni-, dengan jumlah yang tinggi kobalt dan berbagai jenis memperkuat unsur, paduan ini di 815 ~ 870 ° C memiliki kekuatan tarik tinggi dan kemampuan contravariance, ketahanan oksidasi yang baik dan ketahanan korosi, dingin dan panas bergantian berulang kali di bawah aksi dari kekuatan lelah yang lebih tinggi dan sifat mampu bentuk yang baik dan mampu las. Digunakan untuk hidangan turbin mesin turbin, daun, pengencang suhu tinggi, hoop kartu, segel dan komponen elastis dll

     bahan kimia HY N90: (GB / T14992-2005)

    campuran % Ni cr  Fe Zr  B  Bersama C M N si  S  cu  Al Ti
    HY N90 Min bal 18.0 15.0 1,0 2.0
    Max 21.0 1.5 0,15  0.02 21.0 0.13 0,4 0.8 0,015 0,2 2.0 3.0

     kemampuan fisik HY N90:

    density
    g / cm3
    M.point
    ° C
    Perpindahan panas Tingkat
    λ / (W / m • ° C)
    kapasitas panas spesifik
    J / kg • ° C
    modulus elasticityGPa geser elasticityGPa R
    μΩ • m
    koefisien linear ekspansi
    a / 10-6 ° C-1
    8.2 1400 21,76 (100 ° C) 225 12,7 (20 ~ 100 ° C)

     HY N90 kekuatan ablity:

    Perawatan panas Kekuatan tarik σb / MPa Yield Strength σp0.2 / MPa Elongationσ5 /% HB HBS
    solusi pengobatan 820 590 8

     kinerja proses Nimonic90 dan persyaratan:

    1, paduan dalam menempa mudah menghasilkan dalam crack, memungkinkan pukulan palu, tidak mengizinkan chamfering suhu rendah. Ingot suhu pakaian tungku tidak lebih tinggi dari 700 ° C, 1150 ° C ± pemanasan akhir suhu 10 ° C, terbuka penempaan tidak di bawah 1.060 suhu ° C, dan suhu penempaan tidak kurang dari 950 ° C.

    2, ukuran derajat gabah rata-rata tempa paduan dan tingkat deformasi, akhirnya penempaan terkait erat dengan suhu.

    3, paduan dalam keadaan larutan padat dapat perlindungan gas inert listrik las busur dan tungsten sangat butt flash las.

    Spesifikasi:

    bar/wire

    BS HR2 Nimonic 90 bars, billet, forgings;BS HR501 Nimonic 90 cold drawn wire for springs;BS HR502 Nimonic 90 cold drawn and solution; treated wire for springs;BS HR503 Nimonic 90 wire for thread inserts;AMS 5829;AECMA PrEN 2295;AECMA PrEN 2296;AECMA PrEN 2297;AECMA PrEN 2400;AECMA PrEN 2401;AECMA PrEN 2669;AECMA PrEN 2670;MSRR 7016;MSRR 7137;Siemens DL 1641-1;ABB Stal 63 73 01

    sheet/plate/strip

    BS HR202 Nimonic 90 sheet and strip;MSRR 7087;AECMA PrEN 2298;Siemens TLV8525 2100;Siemens TLV8525 31001

    Tabung

    BS HR 402;AECMA PrEN 2299

     

    bentuk biasa untuk semua jenis paduan
    Bentuk Spesifikasi Form pasokan Lainnya
    Lembar Tebal: 0.40-4.75mm, General Lebar: 1000,1219,1500mm Seluruh Coil atau bagian dari itu Annealed dingin, Surface 2B, 2E
    Piring Tebal: 4.76-60mm, Lebar: 1500,2000,2500mm, Panjang: 3000,6000,8000,8500mm (plate bawah 10mm dapat melingkar) Seluruh Coil atau bagian dari itu Tunggal rolling panas, Solid solusi anil negara, 1D Permukaan
    Sabuk Tebal: 0.10-3.0mm, Lebar: 50-500mm Seluruh Coil atau ukuran Ditentukan Annealed dingin, Surface 2B, 2E
    Bar & Rod Rolled barΦ5-45mm, Length≤1500mm Dipoles Bar (lingkaran, Square) Solusi anil, kerak
    Forged barΦ26-245mm, Length≤4000mm
    tabung las Outer diameterΦ4.76-135mm, Wall Thickness0.25-4.00mm, Panjang: ≤35000 mm Berdasarkan kebutuhan Anda
    seamless Tabung Outer diameterΦ3-114mm, Wall Thickness0.2-4.5mm Berdasarkan kebutuhan Anda
    Kawat Outer diameterΦ0.1-13mm Berdasarkan kebutuhan Anda Ni & Ni, Ti & Ti paduan
    ditempa piece cakram, cincin, kotak, balok, lempeng Berdasarkan kebutuhan Anda Steel, Alloy
    Flangs Semua jenis Flangs Berdasarkan kebutuhan Anda Steel, Alloy
    welding Material Coil kawat Φ0.025mm-1.6mm Berdasarkan kebutuhan Anda Surat Keterangan Asal: Amerika, Swedia, Inggris, Jerman, Austria, Italia, Perancis.
    Lurus WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tabung Siku, tiga link, empat link, ukuran diameter yang berbeda Berdasarkan kebutuhan Anda Ni & Ni, Ti & Ti paduan
    Explosive laminasi terikat Baku Lembar Thickness≥2mm Berdasarkan kebutuhan Anda Ni & Ni, Ti & Ti paduan