Inconel Alloy Inconel 602CA UNSN06025

\

Short Introduction:

HY 602CA/Inconel 602CA  UNSN06025  /W. Nr./EN 2.4633/ERNiCrFe-12

HY  602 CA® alloy is the most oxidation resistant/high strength nickel alloy available. It is capable of extreme temperature use up to and beyond 2200°F (1200°C). For thermal processing applications where minimal product contamination is necessary, the oxidation/scaling resistance of RA 602 CA is extremely desirable. A high chromium content, along with aluminum and yttrium additions, allows the alloy to develop a tightly adhering oxide scale.

A relatively high carbon content combined with the alloying additions of titanium and zirconium results in high creep rupture strength. RA 602 CA provides 150% of the strength of other commonly used nickel alloys such as alloy 600.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY 602CA Material grades and equivalents

    Inconel 602CA  UNSN06025  /W. Nr./EN 2.4633/ERNiCrFe-12

    HY 602CA  Chemical composition:

    Cr Ni C Al Ti Y Zr Mn Si Cu Fe
    MIN 24.00 0.15 1.80 0.10 0.05 0.01 8.00
    MAX 26.00 Balance 0.25 2.40 0.20 0.12 0.10 0.15 0.50 0.10 11.00

     

    Specifications:

    Rod, Bar, Wire and Forging Stock

    ASTM B166; ASME SB166

    Plate, Sheet and Strip

    ASTM B168; ASME SB168

     

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy