Nickel Alloy Incoloy 925 UNS N09925

\

Short Introduction:

HY 925 / 인코 로이 925 / UNSN09925니켈 - 크롬 - 철의 시대 - 경화 합금이다. 몰리브덴 및 구리 내용은 부식성 매체에 대한 내성을 강화하면서 티타늄과 알루미늄의 추가는 나이 경화 할 수 있습니다. 주로 가스의 생산에 애플리케이션을 위해 설계되었습니다.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    Y925 재질 등급과 동등

    HY 925 /UNSN09925

    HY 925화학를 compostion :

    Alloy

    %

    Ni

    Cr

    Fe

    C

    Mn

    Si

    Cu

    S

    Al

    Ti

    P

    Mo

    HY 925

    Min.

    42

    19.5

    1.5

    0.15

    1.9

    2.5

    Max.

    46

    23.5

    0.03

    1

    0.5

    3

    0.03

    0.50

    2.4

    0.03

    3.5

    HY 925 물리적 특성 :

    Density

    8.14 g / cm3

    Melting point

    1343 ℃

    roomtemperature에서 HY 925 최소한의 기계적 특성

    Alloy state

    Tensile strength
    Rm N/mm²

    Yield strength

    RP0.2의 N / mm² 인

    Elongation

    5 %

    Solution treatment

    650

    300

    30

    아래와 같이 HY 925 특징

    이 니켈 - 크롬 - 철의 시대 - 경화 합금이다. 몰리브덴 및 구리 내용은 부식성 매체에 대한 내성을 강화하면서 티타늄과 알루미늄의 추가는 나이 경화 할 수 있습니다. 주로 가스의 생산에 애플리케이션을 위해 설계되었습니다.

    HY 925 응용 분야

    그것뿐만 아니라 고강도 배관 시스템에 사용을 찾는로서는, 가스 웰 요소, 밸브 및 배관 등의 애플리케이션을 위해 석유 산업에서 사용된다.

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy



  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !