Lowest Price for Nickel Alloy Inconel 625 UNS N06625 Wholesale to Uruguay
We thinks what customers think, the urgency of urgency to act in the interests of a customer position of principle, allowing for better quality, lower processing costs, prices are more reasonable, won the new and old customers the support and affirmation for Lowest Price for Nickel Alloy Inconel 625 UNS N06625 Wholesale to Uruguay, winning customers' trust is the gold key to our success! If you are interested in our products, please feel free to visit our web site or contact us.
HY 625 Material grades and equivalents
Inconel 625/ GB NS336 / UNS N06625/ SEW VDIUV W.Nr.2.4856 NiCr22Mo9Nb / BS NA 12 / AFNOR NC22DNB
HY 625 Chemical composition
|
Alloy |
% |
Ni |
Cr |
Mo |
Nb+N |
Fe |
Al |
Ti |
C |
Mn |
Si |
Cu |
P |
S |
|
625 |
Min. |
58 |
20 |
8 |
3.15 |
|||||||||
|
Max. |
23 |
10 |
4.15 |
5 |
0.4 |
0.4 |
0.1 |
0.5 |
0.5 |
0.5 |
0.015 |
0.015 |
HY 625 Pysical properties
|
Density |
8.4 g/cm³ |
|
Melting point |
1290-1350°C |
HY 625 Alloy m inimum mechanical properties in the room temperature
|
Alloy state |
Tensile strength |
Yield strength |
Elongation A 5 % |
Brinell hardness |
|
625 |
760 |
345 |
30 |
≤220 |
Characteristic as below
1. Excellent corrosion resistance of different kinds of media in both oxidation and reduction environments.
2. Excellent resistance of pitting and crevice corrosion, and won’t happen stress corrosion cracking because of chloride.
3.Excellent resistance of the inorganic acid corrosion performance, such as nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid and the mixture of sulfuric acid and hydrochloric acid.
4. Excellent corrosion resistance of different kinds of inorganic acid mixture performance.
5. Good corrosion resistance of a variety of concentrations of hydrochloric acid when the temperature up to 40°C .
6. Good machining and welding, no weld cracking sensitivity.
7. Have pressure vessel authentication for the wall temperature between -196 ~ 450°C .
8. Apply for the highest standard lever VII of acidic environment by the NACE ( MR-01-75) authorized.
HY 625 Corrosion resistance
625 own a very good corrosion resistance in many media, especially with excellent resistance to pitting, crevice corrosion, intercrystalline corrosion, and erode in oxide, also good resistance to inorganic acid corrosion, such as nitric acid, phosphoric acid, sulfuric acid and hydrochloric acid. 625 can resist the alkali and organic acid corrosion in the oxidation and reduction environment. Effect resists the chloride reduction stress corrosion cracking. Normally no corrosion in the sea-water and industry environments since high corrosion resistance to the sea-water and salting liquid,as well as in high temperature, without sensitivity during welding. 625 have the resistance to oxidation and carbonizing in the static and cycle environments, also hacve the resistance the chlorine corrosion.
HY 625 Application field
Soften annealing low carbon alloy 625 widely used in the chemical process industry, good corrosion resistance and high strength made it an good choice for structural parts. 625 have application in sea-water for local mechanical stress attach.
HY 625 Typical application field as below
1 .The Organic chemical process parts contains chloride, especially in the use of acid chloride catalyst.
2. The digester and bleacherin the use of paper pulp and paper making industry.
3.Absorption tower, re-heater,gas import board, fan, blender, fair water fin, flue and so on for using in flue gas desulfurization system.
4. The equipment and parts in the use of acidic gas environments.
5. Acetic acid and anhydride reaction generator
6. Sulfur acid cooling
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Qingdao NPA Marketplace Co. Ltd is a foremost manufacturer specialized in centrifugal casting tube and static castings of warmth resistant alloys, which include ethylene cracking furnace tube, reformer furnace tube, CAL(constant annealing traces) &CGL(constant galvanizing traces) furnace roller and radiant tube, glass lehr roller and warmth/have on resistant castings. The annual potential is 9000 tons centrifugal casting tube and 3500 tons static castings (500 tons precision castings).