Newly Arrival Nickel Alloy Monel K500 UNS N05500 Factory for Greenland
Reliable quality and good credit standing are our principles, which will help us at a top-ranking position. Adhering to the tenet of "quality first, customer supreme" for Newly Arrival Nickel Alloy Monel K500 UNS N05500 Factory for Greenland, we are now looking forward to even greater cooperation with overseas customers based on mutual benefits. If you are interested in any of our products, please feel free to contact us for more details.
HY MK-500 Material grades and equivalents
Monel K-500/W Nr.2.4375/Nickel-Copper Alloy 500/UNS N05500
HY MK-500 Chemical composition:
Alloy |
% |
Ni |
Cu |
Al |
Ti |
Fe |
Mn |
S |
C |
Si |
Monle K500 |
Min. |
63 |
27.0 |
2.30 |
0.35 |
|||||
Max. |
33.0 |
3.15 |
0.85 |
2.0 |
1.5 |
0.01 |
0.25 |
0.5 |
HY MK-500 Physical properties:
Density |
8.44 g/cm3 |
Melting point |
1315-1350℃ |
HY MK-500 minimum mechanical properties in the room temperature:
Forms | Condition | Max. section Thickness,in.(mm) | Tensile strength Min. Ksi.(Mpa) | Yield strength Min.Ksi.(Mpa) | Elongation in 2 in,or 4D,min.,% | Hardness | |
HB min. | HRC min. | ||||||
Round bars, Hexagons, squares, rectangles and forgings | hot-worked and age hardened | All Sizes | 140(965) | 100(690) | 20 | 265 | 27 |
Round bars | cold worked and age hardened | 1/4(6.4)to 1(25.4) | 145(1000) | 110(760) | 15 | 300 | 32 |
over 1(25.4)to 3(76.2) | 140(965) | 100(690) | 17 | 280 | 29 | ||
over 3(76.2)to 4(101.6) | 135(930) | 99(655) | 20 | 255 | 25 | ||
Hexagons | cold worked and age hardened | 1/4(6.4)to 2(50.8) | 140(965) | 100(690) | 15 | 265 | 27 |
Round bars, Hexagons, squares, rectangles and forgings | Annealed and age hardened | Up to 1(25.4) | 130(895) | 90(620) | 20 | 250 | 24 |
1(25.4)and over | 130(895) | 85(585) | 20 | 250 | 24 |
HY MK-500 has approximately twice the tensile strength and triple the yield strength of Alloy 400. The strength of Alloy K-500 is maintained to 1200 degrees Fahrenheit, but stays ductile and tough down to temperatures of -400 degrees Fahrenheit. Alloy K-500 also stays non-magnetic to -200 degrees Fahrenheit.
Additional characteristics of Alloy K-500 include outstanding corrosion resistance in a wide range of chemical and marine surroundings, from salts and alkalis, non-oxidizing acids to pure water. HY MK-500 is non-magnetic and spark resistant. It is also recommended that Alloy K-500 be annealed when it is welded and that any weldments be stress relieved prior to aging.
Industries Served:
gas & oil extractionchemical processingmarine engineering
Regular shape for all kinds of alloys | |||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Check out additional TIG Welding Video clips from Weld.com:
http://www.weld.com/index.php/Mr-Tig-Blog/
Subscribe on YouTube and Never ever Miss a Video!
http://www.youtube.com/channel/UCM0kHJXSHR1k1wtLuliKmHg?sub_confirmation=one
Pay a visit to the Welding Discussion board to Carry on the Dialogue and Compete in Month to month Contests!
http://www.weld.com/index.php/Weekend-Warrior-Welding-Discussion board/groups.html
Fb: https://www.fb.com/WeldDotCom
Twitter: https://twitter.com/WeldDotCom
—————————————————————————–
Weld.com welding films are a collection of welding displays that are loaded with welding strategies, tricks and hints that will support you drop that perfect bead each individual time! Whether you are making an attempt to become far better in the locations of TIG Welding, MIG Welding, Adhere Welding or Slicing Weld.com has what you will need. All films are shot from “guiding the hood” so you can get the welders standpoint. In addition to exhibiting you how to weld, many periods we will clearly show you popular issues and how to steer clear of them.
New episodes each individual Friday!
Early launch on the discussion board!
» Metal Tubes India is a GOVT. OF INDIA Acknowledged STAR EXPORT Dwelling & PED Accredited Maker
» Metal Tubes India is winner of All India Award for export excellence for 6 Consecutive Many years
» Metal Tubes India is an ISO 9001,ISO 14001,OHSAS 18001 Accredited company, our international CRISIL Ranking is SE 2B
» Metal Tubes India is European Force Machines Directive PED-97/23/EC qualified company
Ni 72., Cr fifteen.5, Fe 8. Mn 1. C .fifteen Cu .5 Si .5 S .015
Significant Efficiency Alloys stocks and produces this grade in the adhering to forms: Bar, wire, sheet, plate, coil, fasteners and forgings. Ask for quote on this grade.
Alloy 600 is a nickel-chromium alloy built for use from cryogenic to elevated temperatures in the selection of 2000 deg F(1093 deg C). The superior nickel material of the alloy allows it to retain substantial resistance less than lessening conditions and makes it resistant to corrosion by a range of natural and inorganic compounds. The nickel material gives it exceptional resistance to chloride-ion pressure-corrosion cracking and also offers exceptional resistance to alkaline options.
Inconel 600 Tube
ASME SB-163 ASME SB-516 ASME SB751 AMS 5580
UNS N06600 also offered in numerous forms like cap, elbow, erw pipes, fasteners, fittings, flange, plate, reducer, spherical bar, seamless pipes, sheet, tee and tube at industrial charge.
+ for extra info & specification about Inconel 600 remember to check out
http://www.steeltubesindia.internet/