Permalloy 4J49A /FeNi46Cr5/ Carpenter456/Vacovit 465

\

Short Introduction:

Permalloy 4J49A within a certain range with similar soft glass linear expansion coefficient.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    Permalloy 4J49A Material grades and equivalents

    Trademark

    IMPHY

    ASTM

    VAC

    W.Nr

    4J49A

    FeNi46Cr5

    Carpenter456

    Vacovit 465

    Chemical composition:

    Grade

    C

    Si

    Mn

    S

    P

    Al

    Ni

    Cr

    Fe

    4J49A

    ≤0.03

    0.15-0.3

    0.15-0.3

    ≤0.02

    ≤0.02

    0.1-0.25

    46-48

    5.8-6.5

    Rest

    Characteristic as below:

    Permalloy 4J49A within a certain range with similar soft glass linear expansion coefficient.

    Processing conditions and application:

    In the vacuum industry and the corresponding soft glass matching seal, in which 4J49A, 4J6A CRT cathode cap, vacuum fluorescent display into a column.

    Regular shape for all kinds of alloys

    Form

    Specification

    Supply Form

    Others

    Sheet

    Thickness:0.40-4.75mm,General Width:1000、1219、1500mm

    Whole Coil or piece of it

    Cold Annealed,Surface 2B、2E

    Plate

    Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled)

    Whole Coil or piece of it

    Single hot rolling,Solid solution annealed state,Surface 1D

    Belt

    Thickness:0.10-3.0mm,Width:50-500mm

    Whole Coil or Specified size

    Cold Annealed,Surface 2B、2E

    Bar & Rod

    Rolled barΦ5-45mm,Length≤1500mm

    Polished Bar(circle、Square)

    Solution annealing,descaling

    Forged barΦ26-245mm,Length≤4000mm

    Weld tube

    Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm

    Base on your requirement

    Seamless Tube

    Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm

    Base on your requirement

    Wire

    Outer diameterΦ0.1-13mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Forged piece

    discs,rings,squares,blocks,slabs

    Base on your requirement

    Steel, Alloy

    Flangs

    All kinds of Flangs

    Base on your requirement

    Steel, Alloy

    Welding Material

    Coil wire Φ0.025mm-1.6mm

    Base on your requirement

    Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.

    Straight WireΦ1.6mm-4.0mm

    Welding rodΦ1.2mm-4.0mm

    Tube

    Elbow, three links, four links, different diameter size

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Explosive bonded laminate

    Raw Sheet Thickness≥2mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy