Nickel Alloy Inconel 625 UNS N06625

\

Short Introduction:

HY 625 / Incoenl 625/ GB NS336 / UNS N06625/ SEW VDIUV  W.Nr.2.4856 NiCr22Mo9Nb / BS NA 12 / AFNOR NC22DNB own a very good corrosion resistance in many media, especially with excellent resistance to pitting, crevice corrosion, intercrystalline corrosion, and erode in oxide, also good resistance to inorganic acid corrosion, such as nitric acid, phosphoric acid, sulfuric acid and hydrochloric acid. 625 can resist the alkali and organic acid corrosion in the oxidation and reduction environment.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY 625 Material grades and equivalents

    Inconel 625/ GB NS336 / UNS N06625/ SEW VDIUV  W.Nr.2.4856 NiCr22Mo9Nb / BS NA 12 / AFNOR NC22DNB

     

    HY 625 Chemical composition

    Alloy

    %

    Ni

    Cr

    Mo

    Nb+N

    Fe

    Al

    Ti

    C

    Mn

    Si

    Cu

    P

    S

    625

    Min.

    58

    20

    8

    3.15

    Max.

    23

    10

    4.15

    5

    0.4

    0.4

    0.1

    0.5

    0.5

    0.5

    0.015

    0.015

    HY 625 Pysical properties

    Density

    8.4 g/cm³

    Melting point

    1290-1350°C

    HY 625 Alloy m inimum mechanical properties in the room temperature

    Alloy state

    Tensile strength
    Rm N/mm²

    Yield strength
    R P0. 2N/mm²

    Elongation

    A 5 %

    Brinell hardness
    HB

    625

    760

    345

    30

    ≤220

    Characteristic as below
    1. Excellent corrosion resistance of different kinds of media in both oxidation and reduction environments.

    2. Excellent resistance of pitting and crevice corrosion, and won’t happen stress corrosion cracking because of chloride.

    3.Excellent resistance of the inorganic acid corrosion performance, such as nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid and the mixture of sulfuric acid and hydrochloric acid.

    4. Excellent corrosion resistance of different kinds of inorganic acid mixture performance.

    5. Good corrosion resistance of a variety of concentrations of hydrochloric acid when the temperature up to 40°C .

    6. Good machining and welding, no weld cracking sensitivity.

    7. Have pressure vessel authentication for the wall temperature between -196 ~ 450°C .

    8. Apply for the highest standard lever VII of acidic environment by the NACE ( MR-01-75) authorized.

     

    HY 625 Corrosion resistance

    625 own a very good corrosion resistance in many media, especially with excellent resistance to pitting, crevice corrosion, intercrystalline corrosion, and erode in oxide, also good resistance to inorganic acid corrosion, such as nitric acid, phosphoric acid, sulfuric acid and hydrochloric acid. 625 can resist the alkali and organic acid corrosion in the oxidation and reduction environment. Effect resists the chloride reduction stress corrosion cracking. Normally no corrosion in the sea-water and industry environments since high corrosion resistance to the sea-water and salting liquid,as well as in high temperature, without sensitivity during welding. 625 have the resistance to oxidation and carbonizing in the static and cycle environments, also hacve the resistance the chlorine corrosion.

     

    HY 625 Application field
    Soften annealing low carbon alloy 625 widely used in the chemical process industry, good corrosion resistance and high strength made it an good choice for structural parts. 625 have application in sea-water for local mechanical stress attach.

     

    HY 625 Typical application field as below

    1 .The Organic chemical process parts contains chloride, especially in the use of acid chloride catalyst.

    2. The digester and bleacherin the use of paper pulp and paper making industry.

    3.Absorption tower, re-heater,gas import board, fan, blender, fair water fin, flue and so on for using in flue gas desulfurization system.

    4. The equipment and parts in the use of acidic gas environments.

    5. Acetic acid and anhydride reaction generator
    6. Sulfur acid cooling

     

    Specifications

    Sheet

    AMS 5599/AMS 5879/ASME SB-443 Gr. 1/ASTM B-443 Gr. 1

    Bar

    AMS 5666/ASME SB-446 Gr. 1/ASTM B-446 Gr. 1

    Forging

    AMS 5666/ASME SB-446 Gr. 1/ASTM B-446 Gr. 1

     

     

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy





  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !