Iron Alloy Precision Alloy 4J29 F15

\

Short Introduction:

HY J29/4J29/AISI/ASTM F15/JIS EMAS-1001/W.Nr 1.3912 having similar coefficient of linear expansion with hard glass within a certain temperature range, applied to vacuum industry to match hard glass.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    HY J29 Material grades and equivalents

    4J29/AISI/ASTM F15/JIS EMAS-1001/W.Nr 1.3912

    HY J29 Chemical composition

    Alloy

    %

    Ni

    Cr

    Fe

    Co

    Cu

    C

    Mn

    Si

    P

    S

    Mo

    HY J29

    Min

    28.5

    Rest

    16.8

    Max

    29.5

    0.2

    17.8

    0.20

    0.03

    0.50

    0.30

    0.02

    0.02

    0.20

    HY J29 Alloy Mechanical properties in the room temperature

    Grade

    Average linear expansion factor(10-6℃)

    20℃~100℃

    20℃~300℃

    20℃~400℃

    20℃~450℃

    20℃~500℃

    20℃~530℃

    20℃~600℃

    HY J29

    -

    -

    4.6~5.2

    5.1~5.5

    -

    -

    -

    HY J29 Characteristic as below

    HY J29 having similar coefficient of linear expansion with hard glass within a certain temperature range, applied to vacuum industry to match hard glass.

    Regular shape for all kinds of alloys
    Form Specification Supply Form Others
    Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
    Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
    Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
    Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
    Forged barΦ26-245mm,Length≤4000mm
    Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
    Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
    Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
    Flangs All kinds of Flangs Base on your requirement Steel, Alloy
    Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
    Straight WireΦ1.6mm-4.0mm
    Welding rodΦ1.2mm-4.0mm
    Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
    Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy