Cemented carbide YG6X /UNS C3 /ISO K10、G50 is wear resistance and the use strength are similar to that of YG6. It is used for semi finishing of chilled cast iron, nodular iron, non-ferrous metals and alloys, and also for semi finishing and finishing of high manganese steel, hardened steel and alloy steel.


  • Fob price: US $ 25 - 80 / Kilogram
  • Min.order quantity: 300kg
  • Port: Shanghai
  • Payment terms: L/C,T/T,30% down payment after order, balance against copy of B/L
  • Product Detail

    Product Tags

    YG6X  Material grades and equivalents:UNS C3/ISO K10、G50

    Chemical composition(mass fraction)(%)

    Alloy

    WC

    TiC

    TaC  (NbC)

    Co

    Other

    YG6X

    93.5

    -

    <0.5

    6

    -

    Physical properties &minimum mechanical properties

    Density/ g/cm

    Min Hardness/HRA

    Tensile strength/MPa

    Impact toughness j/cm

    Min Bending strength/ N/cm2

    14.6-15.0

    91

    1400

    -

    1420

    YG6X Characteristic as below:

    The wear resistance and the use strength are similar to that of YG6. It is used for semi finishing of chilled cast iron, nodular iron, non-ferrous metals and alloys, and also for semi finishing and finishing of high manganese steel, hardened steel and alloy steel.

    YG6X Processing conditions and application:

    It is proved that the alloy cast iron alloy cast iron and heat-resistant alloy steel can get good effect, and it is also suitable for the fine processing of ordinary cast iron.

    Regular shape for all kinds of alloys

    Form

    Specification

    Supply Form

    Others

    Sheet

    Thickness:0.40-4.75mm,General Width:1000、1219、1500mm

    Whole Coil or piece of it

    Cold Annealed,Surface 2B、2E

    Plate

    Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled)

    Whole Coil or piece of it

    Single hot rolling,Solid solution annealed state,Surface 1D

    Belt

    Thickness:0.10-3.0mm,Width:50-500mm

    Whole Coil or Specified size

    Cold Annealed,Surface 2B、2E

    Bar & Rod

    Rolled barΦ5-45mm,Length≤1500mm

    Polished Bar(circle、Square)

    Solution annealing,descaling

    Forged barΦ26-245mm,Length≤4000mm

    Weld tube

    Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm

    Base on your requirement

    Seamless Tube

    Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm

    Base on your requirement

    Wire

    Outer diameterΦ0.1-13mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Forged piece

    discs,rings,squares,blocks,slabs

    Base on your requirement

    Steel, Alloy

    Flangs

    All kinds of Flangs

    Base on your requirement

    Steel, Alloy

    Welding Material

    Coil wire Φ0.025mm-1.6mm

    Base on your requirement

    Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.

    Straight WireΦ1.6mm-4.0mm

    Welding rodΦ1.2mm-4.0mm

    Tube

    Elbow, three links, four links, different diameter size

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy

    Explosive bonded laminate

    Raw Sheet Thickness≥2mm

    Base on your requirement

    Ni & Ni alloy, Ti & Ti alloy


  • Previous:
  • Next:

  • Send your message to us:

    INQUIRY NOW
    • * CAPTCHA: Please select the Tree

    RELATED PRODUCTS

    INQUIRY NOW
    • * CAPTCHA: Please select the Tree