铁合金不锈钢17-4PH
HY 17-4PH材料等级和等价物 |
|
||
UNS |
AISI / ASTM |
JIS |
W.Nr |
S17400 |
630,17-4PH |
SUS630 |
1.4542 |
HY 17-4PH化学成分: |
|
|
|
|
|
|
|
|
|||
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
S |
Cu |
Nb |
P |
HY 17-4PH |
Min. |
3 |
15.5 |
平衡 |
|
|
|
|
3 |
0.15 |
|
Max. |
5 |
17.5 |
0.07 |
1 |
1 |
0.03 |
5 |
0.45 |
0.035 |
HY 17-4PH物理性能 |
||
Density |
7.78 /立方厘米 |
|
Melting point |
1400年至1440年℃, |
|
HY 17-4PH最小的室温力学性能 |
||||||
状态 |
Tensile strength |
Yield strength |
Elongation |
HRC(HBS) |
|
|
RM牛顿/平方毫米 |
板Rp0.2牛顿/平方毫米 |
A5% |
|
|
||
480℃的年龄 |
≥1310 |
≥1180 |
≥10 |
≥40 |
|
|
550℃的年龄 |
≥1060 |
≥1000 |
≥12 |
≥35 |
|
|
580℃的年龄 |
≥1000 |
≥865 |
≥13 |
≥31 |
|
|
620℃的年龄 |
≥930 |
≥325 |
≥16 |
≥28 |
|
|
HY 17-4PH特点: |
|
|
|
|
|
||
高强度和硬度,良好的焊接性能和耐腐蚀性 |
|||||||
|
|
|
|
|
|
|
|
HY 17-4PH应用范围和领域: |
|
|
|
|
|||
用于具有高强度和corroson电阻分量 |
|
Regular shape for all kinds of alloys |
|||
Form | Specification | Supply Form | Others |
Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
Forged barΦ26-245mm,Length≤4000mm | |||
Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
Straight WireΦ1.6mm-4.0mm | |||
Welding rodΦ1.2mm-4.0mm | |||
Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |