10% OFF Price For Iron alloy Stainless Steel Nitronic 50 for Anguilla Importers

\

Short Introduction:


Product Detail

Product Tags

We have a highly efficient team to deal with inquiries from customers. Our goal is "100% customer satisfaction by our product quality, price & our team service" and enjoy a good reputation among clients. With many factories, we can provide a wide range of 10% OFF Price For Iron alloy Stainless Steel Nitronic 50 for Anguilla Importers, Standing still today and looking into the future, we sincerely welcome customers all over the world to cooperate with us.


HY Nitronic 50  Material grades and equivalents

UNS

AISI/ASTM

ID

Trademark

S20910

XM-19

Fxm-19

Nitronic50

 HY Nitronic 50 Chemical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

N

Mo

Nb

V

P

S

HY Nitronic 50

Min.

11.5

20.5

52

4

0.2

1.5

0.1

0.1

Max.

13.5

23.5

62

0.06

6

1

0.4

3

0.3

0.3

0.04

0.03

 HY Nitronic 50 Physical properties

Density

7.8g/cm3

Melting point

1415-1450 °C

 HY Nitronic 50 Alloy mi nimum mechanical properties in the room temperature

Alloy status

Tensile strength

Rm N/mm²

Yield strength

RP0.2 N/mm²

Elongation

A5 %

Brinell hardness

HB

Solution treatment

690

380

35

≤241

 HY Nitronic 50 Characteristic:

HY Nitronic 50 Stainless Steel provides a combination of corrosion resistance and strength not found in any other commercial material. This austenitic stainless steel has corrosion resistance greater than that provided by types 316, 316L, 317, 317L plus approximately twice the yield strength at room temperature. In addition, HY Nitronic 50 has very good mechanical properties at both elevated and sub-zero temperatures unlike many austenitic stainless steel grades.

HY Nitronic 50 does not become magnetic in cryogenic situations.

High Strength (HS) Nitronic 50 has a yield strength about three times that of 316 Stainless Steel.

HY Nitronic 50 Application field:

Used in petroleum, petrochemical, manure, chemical, nuclear fuel recycle, paper making, textile and food processing industries parts of furnace, combustion chamber, gas turbine and heat-treating facility connecting piece

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy