12 Years Factory wholesale Titanium alloy 6Al-4V UNS R56400 for Naples Factory
We are ready to share our knowledge of marketing worldwide and recommend you suitable products at most competitive prices. So Profi Tools offer you best value of money and we are ready to develop together with 12 Years Factory wholesale Titanium alloy 6Al-4V UNS R56400 for Naples Factory, welcomes all overseas friends and merchants to establish collaboration with us. We will provide you with honest, high quality and efficient service to meet your requirements.
HY Titanium 6-4 Material grades and equivalents
6-4 Titanium, 6-4, Ti 6-4, UNS R56400
Introduction
HY Titanium 6-4 is the most widely used of all the alpha-beta titanium alloys. It is typically used in the annealed condition, at service temperatures through 750°F. However it may be heat treated for high strength in sections under 4″ thick. Hardenability is limited and sections over one inch may not develop full properties. HY Titanium 6-4 is welded with matching or with ELI filler wire.
Mill anneal: 1300-1450°F 2 hours, air cool. Recrystallization anneal bar for better ductility and fatigue strength, 1750°F 2 hours, furnace cool.
For maximum fracture toughness and SCC resistance: Beta anneal 1950°F 1-2 hours, water quench. Then age 1150-1300°F 2 to 4 hours, air cool.
For maximum strength: solution-treated and aged (STA) condition is: For sheet, 1675-1725°F 5 to 25 minutes, water quench. Age 975°F 4 to 6 hours, air cool. For bars and forgings, 1675-1725°F 1 hour, water quench. Age 975-1025°F 3 hours, air cool.
For increased fracture toughness, but lower tensile strength: precipitation treat (overage) 1150-1250°F 4 hours, air cool. Stress relief annealing is commonly 1000-1200°F 1 to 4 hours, air cool.
HY Titanium 6-4 is resistant to general corrosion but may be quickly attacked by environments that cause breakdown of the protective oxide. These include hydrofluoric (HF), hydrochloric (HCl), sulfuric and phosphoric acids. Inhibitors may help for the last four but not for HF. HY Titanium 6-4 resists attack by pure hydrocarbons, and most chlorinated and fluorinated hydrocarbons (provided water has not caused formation of small amounts of HCl and HF).
HY Titanium 6-4 is susceptible to chloride stress corrosion cracking (SCC), although being among the better of the titanium alloys in this regard. For marine environments silver plated bolts are not used, as silver bonds easily with chlorine in this environment. HY Titanium 6-4 is also susceptible to SCC in environments such as methyl alcohol, red fuming HNO3, and N2O4. In the case of red fuming nitric acid, the problem is limited to environments containing less than 1.5% water, or more than 6% NO2. Failure in N2O4 has occurred when oxygen and chlorides were present as impurities.
Chemistry Composition
|
|
Al |
V |
C |
N |
O |
H |
Fe |
Y |
Others, |
Others, |
Ti |
|
MIN |
5.5 |
3.5 |
– |
– |
– |
– |
– |
– |
– |
– |
– |
|
MAX |
6.75 |
4.5 |
0.08 |
0.05 |
0.2 |
0.0125 |
0.3 |
0.005 |
0.1 |
0.4 |
Balance |
Features
- High strength to 600°F
- Excellent general corrosion resistance
- High strength-to-weight ratio
Applications
- Turbine blades, discs and rings
- Aircraft structural components
- Weapons structural components
- Fasteners
- Medical and dental implants
- Hand tools
- Sporting equipment
- Chemical process equipment
Physical Properties
Density: 0.160 lb/inch3
Melting Range: 2929 – 3020°F
Beta Transus: 1825± 25°F
|
Temperature, °F |
70 |
200 |
400 |
600 |
|
Coefficient of Thermal Expansion, in/in°F x 10-6 |
- |
5.3 |
5.4 |
5.5 |
|
Thermal Conductivity, |
4.0 |
4.3 |
5.2 |
6.1 |
|
Modulus of Elasticity, |
16.7 |
16.0 |
15.0 |
14.0 |
Mechanical Properties
Specified, AMS 4911, annealed sheet & plate
|
|
Anneal 1300°F, Air Cool |
Anneal 1300°F, Solution anneal 1750°F , Age 1000°F |
|
Ultimate Tensile Strength, ksi |
138-155 |
150-172 |
|
0.2% Yield Strength, ksi |
128-147 |
137-156 |
|
Elongation, % |
15-20 |
15-17 |
|
Reduction of Area, % |
38-51 |
41-46 |
Typical Tensile Strength and Fracture Toughness, Various Heat Treatments for Flat-rolled Products (MCIC-HB-02 1985 reprint)
|
|
0.2% Yield Strength, ksi |
Fracture Toughness K1C, ksi √in |
|
Annealed |
132 |
128 |
|
Beta Annealed (plate) |
131 |
134 |
|
Beta STA 1250°F b |
128 |
150 |
|
Beta STA 1000°F b |
143 |
120 |
|
STA 1250°Fc |
137 |
105 |
|
STA 1000°Fc |
159 |
80 |
(a) Directional variations,
(b) Beta heat treated followed by solution treating and overaging 1250˚F, or aging 1000˚F
(c) Solution treating and overaging 1250˚F, or aging 1000˚F
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.shelmetcastings.com
Get a Totally free Process Suggestion. Get in touch with 920-622-3344
How to locate a reputable expense caster – Getting a reputable expense caster is just not normally straightforward. Look for people who have been in organization a very long time. Look for issues like the ISO seals, due to the fact when expense casters are adhering to the ISO 9000 technique they have committed to a high quality plan. A high quality plan generally suggests you have a reputable caster. Shelmet Financial investment Casting Enterprise, Inc, has been in organization for around 55 a long time and we are ISO 9008 qualified which is portion of the ISO9000 technique. Shelmet Precision Casting, Inc is at the moment evaluating and expecting acceptance on the ISO2015 update. We feel that we are one of the ideal expense casters in the field. Why do we feel that? Simply because we reside it just about every working day. American Manufactured.
Experienced precision casting expense foundries like Shelmet Precision Casting, Inc, generate a selection of metal castings in sizes from fractions of an ounce to 20 kilos or more. Various varieties of expense casting and precision casting have dated again a couple of hundreds of a long time. Pretty much the exact methods of melting metals, producing easy dies for numerous instances, and producing the finished metal casting utilised really comparable tactics very long ago. Remarkably in depth castings make expense castings the ideal decision for manufacturing finished metal castings often generated from various alloys. Artworks of copper and bronze and even gold ended up created using precision casting tactics, due to the fact these metals and easy metal alloys ended up more conveniently available.
Wax Place: sample waxes, soluble waxes, specialty waxes, wax reclamation and recycling products, wax sample cleaner and sample wetting remedy
Refractories: fused silica, tabular alumina, fused brown alumina, alumina silicates, molochite, white alumina, sand & flours, zirconia, plaster, fiber increased refractories and carbon stucco
Binders: binders, silica, gravity chart, wetting agents and other additives
Crucibles: crucibles and pour cups
Metals: scrap and copper, brass, metal, nickel, cobalt and other alloys
Of system each individual casting business will have their very own distinct combinations of casting machines, based on the varieties of metals and alloys they focus in and on regardless of whether their concentration is expense casting, die casting, sand casting or other casting functions.
Remember to call Shelmet Precision Casting for all your casting demands. http://www.shelmetcastings.com
Get a fast estimate now: 920-622-3344
Alloys: three hundred Series Stainless Metal, Aluminum Alloys, Carbon & Lower Alloy Steels, Cobalt Base Alloys, Gray Iron, Nickel Base Alloys (airmelt), Precip. Hardening St. Metal (seventeen-4PH,fifteen-5PH), four hundred Series Stainless Metal, Copper Base Alloys, Device Steels
Some big industries that use Shelmet Precision Castings, Inc:
Agricultural Machinery
Health-related Devices
Foodstuff Processing Devices
Valve and Hydraulics
Electrical Distribution
Waste and Water Therapy Devices
Paper Production and Processing
Mining Devices
Marine Fittings
Financial investment casting machines is the spine of just about every metal casting method. Financial investment casting machines can be divided into two groups, consumables and genuine machines. Devices by itself can be divided by place: wax place, shell place, foundry, ending place and software place. The consumables can be divided by variety: waxes, refractories, binders, crucibles and metals.
How the Aerospace field works by using expense castings?
How to Ask An Expert at No Charge for Your Financial investment
Casting Tasks?
Advantages of etching your expense castings?
How to get no cost method recommendations for your
expense casting projects?
How to Conserve with Financial investment Casting?
How to get the job done with numerous suppliers in Precision Casting?
When to USe Teflon Coating?
Why Anodize a Metallic Casting?
Why Plate a lost wax casting?
Main Products: Aerospace, Architectural Components, Diesel Engines, Firearms, Foodstuff Processing, Typical Vehicles/Tractors, Industrial Fuel Turbines, Marine Purposes, Army Components, Pumps/Valves, Sporting Products, Automotive, Typical Field, Health-related Devices
Financial investment casting parts and structures have substantial toughness and mechanical houses, and are rarely vulnerable to worn out exhaustion. The mechanical houses and micro-structure of the alloys can be conveniently controlled by the location time, as quick cooling tactics produce outstanding toughness casting parts. Financial investment Casting Devices – Metal Financial investment Castings – Shed Wax Castings – All Preferred Metallic Casting Alloys
Shed wax casting
As Found on FOX Company Information with John Criswell, Production Marvels
The manufacturing method will assist you in the genuine mechanical layout. Shed wax casting is the method exactly where a metal alloy is solid from layout prototype.
Latitude-Longitude: forty four.16993,-89.247591
Shelmet Precision Castings, Inc.
http://www.shelmetcastings.com
Get a fast estimate now. Get in touch with 920-622-3344
This is our 4000 watt Co2 laser slicing process. We can cut Stainless Steel and alloys to .five hundred”, Steel and metal alloys to .750″ and aluminum to .375″. Equally our devices have big bed dimensions, just one is sixty” x 120″ and the 3000 watt is seventy eight” x 157″. Equally devices have automatic loading and shuttle tables for prototyping to manufacturing.