We are proud of the high customer satisfaction and wide acceptance due to our persistent pursuit of high quality both on product and service for 13 Years Factory wholesale Iron alloy Stainless Steel Nitronic 60 for Hungary Manufacturers, We sincerely welcome domestic and foreign merchants who calls, letters asking, or to plants to negotiate, we will offer you quality products and the most enthusiastic service,We look forward to your visit and your cooperation.
HY Nitronic 60 Material grades and equivalents
|
UNS |
AISI/ASTM |
|
S21800 |
Alloy218 |
HY Nitronic 60 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
N |
P |
S |
|
HY Nitronic 60 |
Min. |
8 |
16 |
59 |
|
7 |
3.5 |
0.08 |
|
|
|
Max. |
9 |
18 |
66 |
0.1 |
9 |
4.5 |
0.18 |
0.04 |
0.03 |
HY Nitronic 60 Physical properties
|
Density |
8.0g/cm3 |
|
Melting point |
1375°C |
HY Nitronic 60 Alloy minimum mechanical properties in the room temperature
|
Alloy status |
Tensile strength Rm N/mm² |
Yield strength RP0.2 N/mm² |
Elongation A5 % |
Brinell hardness HB |
|
Solution treatment |
600 |
320 |
35 |
≤100 |
HY Nitronic 60 Characteristic
HY Nitronic 60 Stainless Steel provides a significantly lower cost way to fight galling and wear compared with cobalt-bearing and high nickel alloys. Its uniform corrosion resistance is better than type 304 in most media. In HY Nitronic 60 ,chloride pitting is superior to Type 316.
Yield strength at room temperature is nearly twice that of 304 and 316.
HY Nitronic 60 provides excellent high temperature oxidation resistance and low-temperature impact resistance.
HY Nitronic 60 Application field:
Used extensively in the Power, Chemical, Petrochemical, Food and Oil & Gas industries with an array of uses including expansion joint wear plates, pump wear rings, bushings, process valve stems, seals and logging equipment.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.GovLiquidation.com – This 69,560 lbs of Inconel 625 scrap steel has been bought. To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
This Inconel was in matrix roll kind and free in pans. This good deal of significant temp alloy scrap steel consisted of Carbon: max .10%, Chromium: min 20% max 23%, Iron: max 5%, Silicon: max .fifty%, Manganese: max .fifty%, Sulfur: max .015%, Phosphorus: max .015%, Molybdenum: min 8% max 10%, Titanium: max .forty%, Nickel: Stability.
This material was positioned in Anniston, AL.
To look at a current checklist of obtainable scrap steel material, pay a visit to http://bit.ly/jL05Ke currently!
Substantial Temp Nickel Centered & Tremendous Alloys – Mechanical Homes Inconel Round Bar, Plate Sheet Offer – Inconel is designed of Mostly Nickel and a number of other aspects. The origin coming from Supernovas. Inconel is a Tremendous Alloy and Michlin Metals sells Inconel Round Bar, Hex Bar, Flat Bar, Plate, Sheet, Tube and Pipe.