abide by the contract", conforms to the market requirement, joins in the market competition by its high quality as well as provides more comprehensive and excellent service for clients to let them become big winner. The pursue of the company, is the clients' satisfaction for 13 Years Factory wholesale Nickel Alloy Inconel 690 UNS N06690 Manufacturer in Swiss, Welcome to build the well and long standing business relationships with our company to create a glorious future together .customers' satisfaction is our eternal pursuit
HY 690 Material grades and equivalents
Inconel 690 / UNS N06690 / W. Nr. 2.4642
HY 690 Chemical composition:
|
Type |
% Main Chemical Composition % |
|||||||
|
Ni |
Cr |
Fe |
Cu |
C |
Si |
Mn |
S |
|
|
HY 690 |
Rest |
27.0~31.0 |
7.0~11.0 |
≤0.05 |
≤0.05 |
≤0.5 |
≤0.5 |
≤0.015 |
HY 690 Physical properties:
|
Density |
Melting range |
Hardness |
|
|
8.73 |
1338~1380 |
HRC36 |
HY 690 Alloy minimum mechanical properties in the room temperature
|
Condition |
Tensile Strength |
Yield strength |
Elongation |
|
A 5 % |
|||
|
Solution |
690~738 |
334~372 |
44~50 |
HY 690 Characteristic as below
HY 690 alloy is a kind of nickel based wrought super alloy which has excellent resistance to many aqueous medium and ability of high temperature atmosphere erosion. It also has high strength , good stability and excellent characteristics for metallurgical processing.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Provider foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.one,3rd Industrial District XiTou Village SongGang City Bao’An District ShenZhen Town GuangDong Province China
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,Third Industrial District XiTou Village SongGang City Bao’An District ShenZhen Metropolis GuangDong Province China