13 Years Manufacturer Nickel Alloy Hastelloy C UNS N06003 Wholesale to Jersey
We stick to the principle of "quality first, service first, continuous improvement and innovation to meet the customers" for the management and "zero defect, zero complaints" as the quality objective. To perfect our service, we provide the products with the good quality at the reasonable price for 13 Years Manufacturer Nickel Alloy Hastelloy C UNS N06003 Wholesale to Jersey, With a wide range, good quality, reasonable prices and good service, we will be your best business partner. We welcome new and old customers from all walks of life to contact us for future business relationships and achieving mutual success!
HY HC Chemical composition
| Alloy |
% |
Ni |
Cr |
Mo |
Fe |
W |
Co |
C |
Mn |
Si |
V |
P |
S |
|
C |
Min. |
balance |
14.5 |
15 |
4 |
3 |
|||||||
|
Max. |
16.5 |
17 |
7 |
4.5 |
2.5 |
0.08 |
1 |
1 |
0.35 |
0.04 |
0.03 |
||
|
C22 |
Min. |
balance |
20 |
12.5 |
2 |
2.5 |
|||||||
|
Max. |
22.5 |
14.5 |
6 |
3.5 |
2.5 |
0.02 |
0.5 |
0.08 |
0.35 |
0.02 |
0.02 |
HY HC Physical properties
|
Density |
8.9 g/cm3 |
|
Melting point |
1325-1370 °C |
HY HC Alloy minimum mechanical properties in the room temperature
| Alloy state |
Tensile strength Rm N/mm2 |
Yield strength R P 0.2 N/mm2 |
Elongation A 5 % |
|
Hastelloy C22 |
690 |
283 |
40 |
Characteristic as below
HY HC is a omnipotent of nickel, chromium and molybdenum mixed alloy, with better corrosion resistance performance than other alloys, for example, Hastelloy C276 alloy, C4 alloy and 625 alloy. HY HC have a good resistance performance to pitting, crevice corrosion and stress corrosion cracking, have excellent inoxidability water medium performance, including the wet-chlorine, nitric acid or oxidizing acid mixed acid with chloride ion. Meantime, HY HC possesses perfect resistance to reduction and oxidation of processing enviroments, then it can be used in some complicated environment or with many different manufacture target factory depend on the omnipotent performance. HY HC possess prominent resistance performance to different chemical environments, including strong oxidizing matter, such as iron chloride, copper chloride, chlorine, heat pollution liquid(organic and inorganic), formic acid, acetic acid, acetyl oxide, sea water and salting liquid and so on.
HY HC Metallurgical structure
HY HC is face-centered cubic lattice structure.
HY HC Corrosion resistance
HY HC alloy suit for many kinds of chemical process industry which contain the oxidizing medium and reductant. High molybdenum and chromium content make it can resist the chloride corrosion, and tungsten make this corrosion resistance better. HY HC is one of a few material that can resist the corrosion of moist chlorine, hypochlorite and chlorine dioxide, this alloyhave prominent corrosion resistanceto high concentration chlorate( iron chloride and copper chloride)
HY HC Application field
HY HC is widely used in the chemical field and petrifaction field, such as the element of chloride organic and catalyze system. This material especially suit for high temperature environments, impure inorganic acid and organic acid (such as formic acid and acetic acid), sea-water corrosion environments.
HY HC Other application field
1. Acetic acid/acetyl oxide
2.Acid dipping
3.Cellophane paper manufactures
4.Chloride system
5. Complicated mixed acid
6. Electrogalvanizing groove roller
7.Expansion bellows
8.Flue gas washer system
9.Geothermal well
10.Fluorine hydride furnace cleaner
11.Incineration cleaner system
12. Nuclear fuel regeneration
13. Pesticide manufacture
14.Phosphoric acid manufacture
15.Acid cleaning system
16.Plate heat exchanger
17. Selectivity filter system
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
NEW 2016 Chrysler three hundred S Alloy Edition Sedan with a Gloss Black Paint finish. AWD that seats five with a three.two L V-six engine and an eight velocity computerized transmission. 19″ alluminum alloy rims with Michelin Primacy MXM4 tires. This sedan will come thoroughly loaded with keyless entry, distant get started, power locks, home windows, mirrors, Beats by Dre audio system, AM/FM, Sirius Sat radio, Lcd display screen in the entrance with back up digicam, leather all over with heated entrance and rear seats and so significantly a lot more. Come check out it out at Ponoka Chrysler and see what else it has to present, we are located on the south conclusion of Ponoka just off of HWY 2A.
Stock# 16C37644
Sarah Johnson,
Ponoka Chrysler
6510 39th Ave Ponoka, AB T4J 1J8
Toll Cost-free: 1(800) 265-6851
Cellphone: (403) 783-5383
Fax: (403) 783-8140
E-mail: sjohnson@ponokachrysler.com
Like us on Fb- https://www.facebook.com/PonokaChrysler/
Abide by us on Instargram- https://www.instagram.com/ponokadodge/
Abide by us on Twitter- https://twitter.com/PonokaDodgeRam
Abide by us on Pintrest- https://www.pinterest.com/ponokachrysler/