18 Years Factory Iron alloy Stainless Steel Nitronic 50 Export to Russia
We insist on the principle of development of 'High quality, Efficiency, Sincerity and Down-to-earth working approach' to provide you with excellent service of processing for 18 Years Factory Iron alloy Stainless Steel Nitronic 50 Export to Russia, We are confident to make great achievements in the future. We are looking forward to becoming one of your most reliable suppliers.
HY Nitronic 50 Material grades and equivalents
|
UNS |
AISI/ASTM |
ID |
Trademark |
|
S20910 |
XM-19 |
Fxm-19 |
Nitronic50 |
HY Nitronic 50 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
N |
Mo |
Nb |
V |
P |
S |
|
HY Nitronic 50 |
Min. |
11.5 |
20.5 |
52 |
4 |
0.2 |
1.5 |
0.1 |
0.1 |
||||
|
Max. |
13.5 |
23.5 |
62 |
0.06 |
6 |
1 |
0.4 |
3 |
0.3 |
0.3 |
0.04 |
0.03 |
HY Nitronic 50 Physical properties
|
Density |
7.8g/cm3 |
|
Melting point |
1415-1450 °C |
HY Nitronic 50 Alloy mi nimum mechanical properties in the room temperature
|
Alloy status |
Tensile strength Rm N/mm² |
Yield strength RP0.2 N/mm² |
Elongation A5 % |
Brinell hardness HB |
|
Solution treatment |
690 |
380 |
35 |
≤241 |
HY Nitronic 50 Characteristic:
HY Nitronic 50 Stainless Steel provides a combination of corrosion resistance and strength not found in any other commercial material. This austenitic stainless steel has corrosion resistance greater than that provided by types 316, 316L, 317, 317L plus approximately twice the yield strength at room temperature. In addition, HY Nitronic 50 has very good mechanical properties at both elevated and sub-zero temperatures unlike many austenitic stainless steel grades.
HY Nitronic 50 does not become magnetic in cryogenic situations.
High Strength (HS) Nitronic 50 has a yield strength about three times that of 316 Stainless Steel.
HY Nitronic 50 Application field:
Used in petroleum, petrochemical, manure, chemical, nuclear fuel recycle, paper making, textile and food processing industries parts of furnace, combustion chamber, gas turbine and heat-treating facility connecting piece
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Inconel – Nickel Dependent Super Alloy – 600, 625, 718, X-750 Qualities and Programs August 2013 Inconel is a tremendous alloy and mixes effectively with Copper. Inconel arrives in a lot of varieties: Round Bar, Plate, Sheet, Pipe, Tube. Inconel is hard to machine for the reason that it perform hardens, Inconel 625 can be welded a bit.
A nitinol wire/form memory alloy inchworm that walks across a table employing only warmth. The warmth is supplied by electrical existing heating up the skinny nitinol wire, causing it to return to its remembered form, a compressed coil in this scenario. A V-formed spring returns it to the commencing form.
Guidance RimstarOrg on Patreon https://www.patreon.com/user?u=680159
Subscribe for new films every single week http://www.youtube.com/user/rimstarorg?sub_affirmation=1
Go to the principal channel webpage below https://youtube.com/rimstarorg
See also:
How to Make Nitinol Wire Inchworm (Shape Memory Alloy)
https://www.youtube.com/look at?v=getfzfZJjHM
Nitinol Wire – How to Use it
https://www.youtube.com/look at?v=4Yi4epJ83EE
How a Rocket Performs/Earth to Area Eg SpaceX Falcon 9 and Dragon
https://www.youtube.com/look at?v=L0AMQ6kRNMA
My webpage about this nitinol wire inchworm:
http://rimstar.org/science_electronics_tasks/nitinol_wire_inchworm_form_memory_alloy_handmade.htm
Adhere to at the rear of-the-scenes on:
Twitter https://twitter.com/#!/RimStarz
Google+ https://additionally.google.com/116395125136223897621
Fb https://www.fb.com/rimstarorg
http://rimstar.org
The inspiration came from this one:
https://www.youtube.com/look at?v=DW4WaTmoZ3c
Essence – audio by audionautix.com