18 Years Factory Pure nickel Alloy Nickel 201 UNS N02201 Export to Peru

\

Short Introduction:


Product Detail

Product Tags

With our excellent management, strong technical capability and strict quality control system, we continue to provide our clients with reliable quality, reasonable prices and excellent services. We aim at becoming one of your most reliable partners and earning your satisfaction for 18 Years Factory Pure nickel Alloy Nickel 201 UNS N02201 Export to Peru, We, with great passion and faithfulness, are willing to provide you with perfect services and striding forward with you to create a bright future.


Material grades and equivalents

Nickel 201 /N02201/ W.Nr 2.4061

HY N201Chemical composition

Alloy

%

Ni

Fe

C

Mn

Si

Cu

S

HY N201

Min.

Balance

Max.

0.4

0.02

0.35

0.35

0.25

0.01

HY N201Pysical properties

Density

8.89 g/cm³

Melting point

1440℃

HY N201 Alloy minimum mechanical properties in the room temperature

Product Form

Condition

Tensile strength
Rm N/mm²

Yield strength
RP0.2 N/mm²

Elongation

A5 %

Brinell hardness
HB

Rod & Bar

Hot Finished

60-85

15-45

35-55

45-80

Rod & Bar

Cold Drawn/Annealed or Hot-Finished/Annealed

55-75

15-30

40-55

45-70

Plate

Hot-Rolled/Annealed

55-80

15-40

40-60

45-75

Sheet

Annealed

55-75

15-30

40-55

70 max

Tube & Pipe

Seamless Annealed

55-75

12-30

40-60

70 max

HY N201Characteristic as below:

Highly resistant to various reducing chemicals

Excellent resistance to caustic alkalies

High electrical conductivity

Excellent corrosion resistance to distilled and natural waters

Resistance to neutral and alkaline salt solutions

Excellent resistance to dry fluorine

Widely used to handle caustic soda

Good thermal, electrical and magnetostrictive properties

Offers some resistance to hydrochloric and sulfuric acids at modest temperatures and concentrations

HY N201 Application field

Food processing equipment

Marine and offshore engineering

Salt production

Caustic handling equipment

Manufacture and handling of sodium hydroxide, particularly at temperatures above 300° F

Reactors and vessels in which fluorine is generated and reacted with hydrocarbons

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS