18 Years manufacturer Iron Alloy Precision Alloy UNS N08031 Alloy 31 to Rwanda Factory
The customer satisfaction is our primary target. We uphold a consistent level of professionalism, quality, credibility and service for
18 Years manufacturer Iron Alloy Precision Alloy UNS N08031 Alloy 31 to Rwanda Factory, Our company will continue to adhere to the " superior quality, reputable, the user first " principle wholeheartedly. We warmly welcome friends from all walks of life to visit and give guidance, work together and create a brilliant future!
HY A31 Material grades and equivalents
AISI/ASTM Alloy 31 / UNS N08031 / W.Nr 1.4562
Chemical composition:
| Alloy | % | Ni | Cr | Fe | Mo | N | C | Mn | Si | 硫 | 铜 | 磷 |
| HY A31 | Min | 30 | 26 | 余量 | 6 | 0.15 | 1 | |||||
| Max | 32 | 28 | 7 | 0.25 | 0.015 | 2 | 0.3 | 0.01 | 1.4 | 0.02 | ||
| Physical properties: | ||||||||||||
| Density | 8.1 g/cm3 | |||||||||||
| Melting point | 1350-1370 ℃ | |||||||||||
| Alloy minimum mechanical properties in the room temperature: | ||||||||||||
| Alloy | Tensile strength Rm N/mm² | Yield strength Rp0.2 N/mm² | Elongation A5 % | |||||||||
| Solution | 650 | 350 | 35 | |||||||||
Characteristic as below:
HY A31 is a nitrogen-containing iron-nickel-molybdenum alloy performance between super austenitic stainless steel and nickel-based alloy, suitable for used in chemical and petrochemical, environment engineering, oil and gas production industrial fields.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Check out additional TIG Welding Video clips from Weld.com:
http://www.weld.com/index.php/Mr-Tig-Blog/
Subscribe on YouTube and Never ever Miss a Video!
http://www.youtube.com/channel/UCM0kHJXSHR1k1wtLuliKmHg?sub_confirmation=one
Pay a visit to the Welding Discussion board to Carry on the Dialogue and Compete in Month to month Contests!
http://www.weld.com/index.php/Weekend-Warrior-Welding-Discussion board/groups.html
Fb: https://www.fb.com/WeldDotCom
Twitter: https://twitter.com/WeldDotCom
—————————————————————————–
Weld.com welding films are a collection of welding displays that are loaded with welding strategies, tricks and hints that will support you drop that perfect bead each individual time! Whether you are making an attempt to become far better in the locations of TIG Welding, MIG Welding, Adhere Welding or Slicing Weld.com has what you will need. All films are shot from “guiding the hood” so you can get the welders standpoint. In addition to exhibiting you how to weld, many periods we will clearly show you popular issues and how to steer clear of them.
New episodes each individual Friday!
Early launch on the discussion board!
.025″ slash, 140sfm, VBMT 331 insert