abide by the contract", conforms to the market requirement, joins in the market competition by its high quality as well as provides more comprehensive and excellent service for clients to let them become big winner. The pursue of the company, is the clients' satisfaction for 2016 Good Quality Cobalt Alloy Stellite 6 UNS R3006 Supply to Abu Dhabi, We welcome you to inquire us by call or mail and hope to build a successful and cooperative relationship.
HY S6 Material grades and equivalents: Stellit 6; UNS R3006; AMS 5387C-2001
Introduction:
HY S6 is the most widely used of the wear resistant cobalt-based alloys and exhibits good all-round performance. It is regarded as the industry standard for general-purpose wear resistance applications.
HY S6 Chemical components
|
C |
Cr |
Si |
W |
Fe |
Mo |
Ni |
Mn |
B |
Co |
|
1.2 |
28 |
1.1 |
4.5 |
3 |
3 |
1 |
bal |
||
| *The chemical composition shown above is an outline only,and should not be taken as a full specification. *Note that cored wire may have higher Fe contents than other product forms. |
|||||||||
HY S6 Physical property (Room Temp.)
| Density (lb/in3) |
Specific Gravity |
Solidus | Liquidus | Specific heat (J/kg·K) |
Magnetic Permeability |
Electrode Potential |
Electrical Conductivity |
Electrical Resistivity |
| 0.305 | 8.46 | 2340°F | 2540°F | 0.101°F Btu/lb- |
<1.2@200 Oersteds |
-0.25 Volts |
1.9%IACS (Int. Annealed Copper Std.) |
41.73 microhms-inch |
HY S6 Thermal Properties-Conductivity & Expansion
| Thermal Expansion Coefficient | Thermal Conductivity by Temperature | ||||||
| °F | Microinch/ inch-°F |
°C | Microns/ m-°C |
°F | Btu/ft2/in/ hr/°F |
°C | W/mk |
| 212 | 6.3 | 100 | 11.34 | 70 | 102.7 | 21.11 | 14.82 |
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html
How to weld nickel alloys like hastelloy, inconel, etc. Nickel alloys have a low thermal conductivity and so limiting heat input and using lower amperage than would be used for stainless is one key to making good nickel alloy welds.
Inconel – Nickel Dependent Super Alloy – 600, 625, 718, X-750 Qualities and Programs August 2013 Inconel is a tremendous alloy and mixes effectively with Copper. Inconel arrives in a lot of varieties: Round Bar, Plate, Sheet, Pipe, Tube. Inconel is hard to machine for the reason that it perform hardens, Inconel 625 can be welded a bit.