2016 Good Quality Nickel Alloy Incoloy 800 UNS N08800 for Lesotho Manufacturer
Our company insists all along the quality policy of "product quality is base of enterprise survival; customer satisfaction is the staring point and ending of an enterprise; persistent improvement is eternal pursuit of staff" and the consistent purpose of "reputation first, customer first" for 2016 Good Quality Nickel Alloy Incoloy 800 UNS N08800 for Lesotho Manufacturer, we have built a reliable reputation among many customers. Quality&customer first are always our constant pursuit. We spare no efforts to make better products. Look forward to long-term cooperation and mutual benefits!
HY 800
Material grades and equivalents
Incoloy 800/GB NS111/UNS N08800/SEW VDIUV W.Nr.1.4876 X10NiCrAlTi3220/BS NA15/AFNOR Z8NC32.21
HY 800 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
S |
Al |
Ti |
|
800 |
Min. |
30 |
19 |
0.15 |
0.15 |
||||||
|
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
|
800H |
Min. |
30 |
19 |
0.05 |
0.15 |
0.15 |
|||||
|
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
|
800HT |
Min. |
30 |
19 |
0.06 |
0.15 |
0.15 |
|||||
|
Max. |
35 |
23 |
balance |
0.1 |
1.5 |
1 |
0.75 |
0.015 |
0.6 |
0.6 |
|
|
AI+Ti: 0.85-1.20 |
|||||||||||
HY 800 Physical properties
|
Density |
8.0 g/cm³ |
|
Melting point |
1350-1400 °C |
HY 800 Alloy minimum mechanical properties in the room temperature
|
Alloy |
Tensile strength |
Yield strength |
Elongation |
|
Rm N/mm² |
R P 0. 2N/mm² |
A 5 % |
|
|
800 |
500 |
210 |
35 |
|
800H |
450 |
180 |
35 |
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Discovery and Science Channel’s How It truly is Designed Alloy Wheels episode.
All copyrights go to their respective homeowners.