abide by the contract", conforms to the market requirement, joins in the market competition by its high quality as well as provides more comprehensive and excellent service for clients to let them become big winner. The pursue of the company, is the clients' satisfaction for 2016 Latest Design Titanium alloy 6Al-4V ELI UNS R56401 Manufacturer in Nairobi, With the aim of "compete with good quality and develop with creativity" and the service principle of "take customers' demand as orientation", we will earnestly provide qualified products and good service for domestic and international customers.


HY Titanium 6-4 ELI Material grades and equivalents

6-4 ELI Titanium, 6-4 ELI, UNS R56401

Introduction

Low interstitial version of HY Titanium 6-4 ELI, for maximum toughness. Preferred for marine and cryogenic applications. This grade is normally used in the annealed condition. HY Titanium 6-4 ELI is the preferred choice for the medical implant field.

Stress relief 900-1200°F 1 to 4 hours, air cool. Duplex anneal, bar and forgings: Solution anneal 50-100°F below the beta transus, hold 1 hour minimum, air cool. Then reheat within the range 1300-1400°F, hold 1 hour minimum, air cool. Stress – relief annealing is performed after welding.

Chemistry Composition

Al

V

Fe

O

C

N

H

Y

Others,
Each

Others,
Total

Ti

MIN

5.5

3.5

MAX

6.5

4.5

0.25

0.13

0.08

0.03

0.0125

0.005

0.1

0.4

Balance

Features

Resistant to bodily fluidsResistant to a variety of corrosive environmentsFreedom from chloride stress corrosion crackingGood strength and toughness over a wide temperature rangeHigh resistance to erosion corrosion and corrosion fatigueUseful resistance to dry chlorine, fluorine, hydrogen chloride and hydrogen fluoride gases

Applications

Medical and dental implantsCryogenicsAerospaceChemical processing

Physical Properties

Density: 0.160 lb/in3
Melting Range: 2370 – 2460°F
Beta Transus: 91790+25°F

Minimum Tensile Properties, AMS 4919, Duplex Annealed

Temperature, °F

68-212

68-600

68-1000

68-1200

68-1500

Coefficient* of Thermal Expansion, in/in°F x 10-6

9.18

9.54

10.08

10.44

10.8

Mechanical Properties

Typical hardness Rockwell: C 30-34 Specific minimums, AMS 4931, bar and forging

Representative Tensile Properties, Sheet

Diameter, in

< 3.0

< 3.0 < 4.0

< 4.0) < 6.0

Tensile Strength, ksi

125

123

120

0.2 % Yield Strength, ksi

115

110

110

Elongation, % *L (**ST)

10 (8)

10 (8)

8 (8)

Reduction of Area, % *L (**ST)

25 (–)

20 (15)

15 (15)

* Longitudinal ** Short Transverse

Typical Elevated temperature Properties

Temperature, °F

93 (200)

149 (300)

204 (400)

260 (500)

Ultimate Tensile Strength, ksi

843.3 (121)

772.2 (112)

723.9 (105)

657.7 (98)

0.2 % Yield Strength, ksi

710.2 (103)

641.2 (93)

586.1 (85)

531.0 (77)

Elongation, %

13

15

16

16

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !