2016 New Style Nickel Alloy Incoloy 825 UNS N08825 Supply to Argentina
We take "customer-friendly, quality-oriented, integrative, innovative" as objectives. "Truth and honesty" is our management ideal for 2016 New Style Nickel Alloy Incoloy 825 UNS N08825 Supply to Argentina, Please send us your specifications and requirements, or feel free to contact us with any questions or inquiries that you may have.
HY 825
Material grades and equivalents
Incoloy 825/GB NS1402/UNS N08825/SEW VDIUV W.Nr.2.4858 NiCr21Mo/BS NA16/AFNOR NC21FeDU
HY 825Chemical composition
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
Mo |
Al |
Ti |
P |
S |
|
825 |
Min. |
38 |
19.5 |
balance |
1.5 |
2.5 |
1.0 |
0.6 |
|||||
|
Max. |
46 |
23.5 |
balance |
0.05 |
1 |
0.5 |
3 |
3.5 |
0.2 |
1.2 |
0.02 |
0.03 |
HY 825Physical properties
|
Density |
8.1 g/cm3 |
|
Melting point |
1370-1400°C |
HY 825Alloy mi nimum mechanical properties in the room temperature
|
Alloy state |
Tensile strength |
Yield strength |
Elongation |
Brinell hardness |
|
825 |
550 |
220 |
30 |
≤200 |
Characteristic as below
1. Good stress corrosion cracking resistance performance
2. Good resistance for pitting and crevice corrosion performance
3. Good anti-oxidation and non-oxidzing heat acid performance
4. Good mechanical performance in both room temperature and up to 550°C
5. Have the pressure vessel authenticate when manufacture temperature up to 450°C
HY 825Metallurgical structure
825 is the face-centered cubic lattice structure.
HY 825Corrosion resistance
825 is an all-purpose project alloy, have good corrosion resistance of the acid and alkali metal property in both oxidation and reduction environments. High nickel content made it with effective stress corrosion cracking resistance performance. 825 have excellent corrosion resistance in different kinds of media, such as sulfuric acid, phosphoric acid, nitric acid and organic acid, alkali metal such as sodium hydroxide, potassium hydroxide, and hydrochloric acid. A variety of media corrosion of nuclear-burning dissolver show 825 high integrated prpperty, like sulfuric acid, nitric acid and potassium hydroxide are all dealing in a same device.
HY 825Application field
825widely use in many kinds of industry field that the working temperature no more than 550°C.
HY 825Typical application field
1. Sulfuric acid factory usage for heating pipe, container, basket, chain and so on.
2. Cooling heat exchanger, marine product pipeline system and gas pipeline of acidic environment.
3. Heat exchanger, steam machine, washing, impregnation pipe, etc. for phosphoric acid produce
4. Oil refining in the air heat exchanger
5. Food project
6. Chemical process
7. Application of high pressure oxygen flam-retardant alloy
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Qingdao NPA Marketplace Co. Ltd is a foremost manufacturer specialized in centrifugal casting tube and static castings of warmth resistant alloys, which include ethylene cracking furnace tube, reformer furnace tube, CAL(constant annealing traces) &CGL(constant galvanizing traces) furnace roller and radiant tube, glass lehr roller and warmth/have on resistant castings. The annual potential is 9000 tons centrifugal casting tube and 3500 tons static castings (500 tons precision castings).
Internet site: www.npa-china.com
Inconel 718, The Severe Metal Alloy. http://www.techsteel.web/alloy/nickel/inconel-718
Turbine Blades have revolutionized air vacation and electricity era.
Hundreds of slim precision blades spinning at a hundred,000 RPM have to have a materials that can stand up to excessive disorders.
Inconel 718 is a distinctive metal alloy that can stand up to excessive temperatures from -423° to 1300°F
This alloy is aged hardened, making it possible for it to be welded without having hardening for the duration of heating and cooling.
The improvement of Inconel began in the fifties for use in vital steam line plants. Originally used for armed service programs it was later on adopted by the professional sector.
Inconel 718‘s tolerance for excessive temperature make it specially perfectly suited for programs such as
turbine blades
nuclear electricity plants, and
aerospace programs. It was used in the space shuttles high force pump.
AMS 5589 | AMS 5596 | AMS 5597 | AMS 5663 | AMS 5664