2016 New Style Pure nickel Alloy Nickel 201 UNS N02201 in Uganda

\

Short Introduction:


Product Detail

Product Tags

Our company puts emphasis on the management, the introduction of talented personnel, and the construction of staff building, trying hard to improve the quality and liability consciousness of staff members. Our company successfully attained IS9001 Certification and European CE Certification of 2016 New Style Pure nickel Alloy Nickel 201 UNS N02201 in Uganda, Adhering to the business principle of mutual benefits, we have won good reputation among our customers because of our perfect services, quality products and competitive prices. We warmly welcome customers from home and abroad to cooperate with us for common success.


Material grades and equivalents

Nickel 201 /N02201/ W.Nr 2.4061

HY N201Chemical composition

Alloy

%

Ni

Fe

C

Mn

Si

Cu

S

HY N201

Min.

Balance

Max.

0.4

0.02

0.35

0.35

0.25

0.01

HY N201Pysical properties

Density

8.89 g/cm3

Melting point

1440℃

HY N201 Alloy minimum mechanical properties in the room temperature

Product Form

Condition

Tensile strength
Rm N/mm2

Yield strength
RP0.2 N/mm2

Elongation

A5 %

Brinell hardness
HB

Rod & Bar

Hot Finished

60-85

15-45

35-55

45-80

Rod & Bar

Cold Drawn/Annealed or Hot-Finished/Annealed

55-75

15-30

40-55

45-70

Plate

Hot-Rolled/Annealed

55-80

15-40

40-60

45-75

Sheet

Annealed

55-75

15-30

40-55

70 max

Tube & Pipe

Seamless Annealed

55-75

12-30

40-60

70 max

HY N201Characteristic as below:

Highly resistant to various reducing chemicals

Excellent resistance to caustic alkalies

High electrical conductivity

Excellent corrosion resistance to distilled and natural waters

Resistance to neutral and alkaline salt solutions

Excellent resistance to dry fluorine

Widely used to handle caustic soda

Good thermal, electrical and magnetostrictive properties

Offers some resistance to hydrochloric and sulfuric acids at modest temperatures and concentrations

HY N201 Application field :

Food processing equipment

Marine and offshore engineering

Salt production

Caustic handling equipment

Manufacture and handling of sodium hydroxide, particularly at temperatures above 300° F

Reactors and vessels in which fluorine is generated and reacted with hydrocarbons

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS