2016 Super Lowest Price Nickel Alloy Inconel 686 UNS N06686 to French Importers

\

Short Introduction:


Product Detail

Product Tags

We insist on the principle of development of 'High quality, Efficiency, Sincerity and Down-to-earth working approach' to provide you with excellent service of processing for 2016 Super Lowest Price Nickel Alloy Inconel 686 UNS N06686 to French Importers, Welcome to build the well and long standing business relationships with our company to create a glorious future together .customers' satisfaction is our eternal pursuit


HY 686 Material grades and equivalents

Inconel 686 / UNS N06686 / Werkstoff Nr.2.4606

HY 686 Chemical composition:

Type

% Main Chemical Composition %

Mo

Cr

Fe

W

C

Si

Mn

P

S

Ti

Ni

HY 686

15.0~17.0

19.0~23.0

≤5.0

3.0~4.4

≤0.01

≤0.08

≤0.75

≤0.04

≤0.02

0.02-0.25

Rest

HY 686 Physical properties

Density Melting range Hardness
8.73 1338~1380 HRC36

HY 686 Alloy minimum mechanical properties in the room temperature

Condition

Tensile Strength

Yield strength

Elongation

Rm N/mm²

R P 0. 2N/mm²

A 5 %

Solution

690

380

45

Cold Drawing/Hot Rolled

1115

1020

23.1

HY 686 Characteristic as below

HY 686 is solid solution strengthening and corrosion resistance nickel based alloy of NI-Cr-Mo, which has good corrosion resistance in severe corrosive environment. They mainly apply to heat exchanger, reaction container and delivery pipe in the area of chemical processing, processing, pollution control, papermaking, industry and garbage treatment etc.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy