2016 Super Lowest Price Nickel Alloy Inconel 690 UNS N06690 Wholesale to Iraq

\

Short Introduction:


Product Detail

Product Tags

Innovation, quality and reliability are the core values of our company. These principles today more than ever form the basis of our success as an internationally active mid-size company for 2016 Super Lowest Price Nickel Alloy Inconel 690 UNS N06690 Wholesale to Iraq, We sincerely welcome all guests to set up business relationships with us on the basis of mutual benefits. Please contact us now. You will get our professional reply within 8 hours.


HY 690 Material grades and equivalents

Inconel 690 / UNS N06690 / W. Nr. 2.4642

HY 690 Chemical composition:

Type

% Main Chemical Composition %

Ni

Cr

Fe

Cu

C

Si

Mn

S

HY 690

Rest

27.0~31.0

7.0~11.0

≤0.05

≤0.05

≤0.5

≤0.5

≤0.015

HY 690 Physical properties:

Density

Melting range

Hardness

8.73

1338~1380

HRC36

HY 690 Alloy minimum mechanical properties in the room temperature

Condition

Tensile Strength
Rm N/mm2

Yield strength
R P 0. 2N/mm2

Elongation

A 5 %

Solution

690~738

334~372

44~50

HY 690 Characteristic as below

HY 690 alloy is a kind of nickel based wrought super alloy which has excellent resistance to many aqueous medium and ability of high temperature atmosphere erosion. It also has high strength , good stability and excellent characteristics for metallurgical processing.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !