24 Years Factory Iron Alloy Precision Alloy 1J79 Alloy4 for Bolivia Manufacturers
Our development depends on the advanced equipment, excellent talents and continuously strengthened technology forces. 24 Years Factory Iron Alloy Precision Alloy 1J79 Alloy4 for Bolivia Manufacturers, We warmly welcome customers from all over the world for any kind of cooperation with us to build a mutual benefit future. We are devoting ourselves wholeheartedly to offer customers the best service.
HY J79 Material grades and equivalents
1J79 / AISI/ASTM Alloy4
HY J79 Chemical composition
|
Grade |
C |
P |
S |
Mn |
Ni |
Si |
Mo |
Cu |
Fe |
||||
|
≤ |
|||||||||||||
| HY J79 |
0.03 |
0.02 |
0.02 |
0.6-1.1 |
78.5-80.5 |
0.3-0.5 |
3.8-4.1 |
≤0.20 |
Rest |
||||
HY J79 Alloy Mechanical properties in the room temperature
|
Grade |
Shape |
Magnetic properties |
|||
|
Initial permeabilityμO |
Maximum permeabilityμm |
Hc |
Saturation induction density BS |
||
|
HY J79 |
Cold rolling strips |
≥31 |
≥250 |
≤1.2 |
0.75 |
|
Rod wire |
≥25 |
≥3125 |
≤2.4 |
0.75 |
|
HY J79 Characteristic as below
HY J79 has a high initial permeability, to work in a weak magnetic field of various transformers, transformers, magnetic amplifiers, choke coil core and magnetic shielding.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html
How to weld nickel alloys like hastelloy, inconel, etc. Nickel alloys have a low thermal conductivity and so limiting heat input and using lower amperage than would be used for stainless is one key to making good nickel alloy welds.