30% OFF Price For Iron alloy Stainless Steel 17-4PH for Zimbabwe Factory
We believe in: Innovation is our soul and spirit. Quality is our life. Customer need is our God for 30% OFF Price For Iron alloy Stainless Steel 17-4PH for Zimbabwe Factory, winning customers' trust is the gold key to our success! If you are interested in our products, please feel free to visit our web site or contact us.
|
HY 17-4PH Material grades and equivalents |
|
||
|
UNS |
AISI/ASTM |
JIS |
W.Nr |
|
S17400 |
630,17-4PH |
SUS630 |
1.4542 |
|
HY 17-4PH Chemical composition: |
|
|
|
|
|
|
|
|
|||
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
S |
Cu |
Nb |
P |
|
HY 17-4PH |
Min. |
3 |
15.5 |
balance |
|
|
|
|
3 |
0.15 |
|
|
Max. |
5 |
17.5 |
0.07 |
1 |
1 |
0.03 |
5 |
0.45 |
0.035 |
||
|
HY 17-4PH Physical properties |
||
|
Density |
7.78/cm3 |
|
|
Melting point |
1400-1440 °C |
|
|
HY 17-4PH Minimum mechanical properties in the room temperature |
||||||
|
Status |
Tensile strength |
Yield strength |
Elongation |
HRC(HBS) |
|
|
|
Rm N/mm² |
Rp0.2 N/mm² |
A5 % |
|
|
||
|
480°C age |
≥1310 |
≥1180 |
≥10 |
≥40 |
|
|
|
550°C Age |
≥1060 |
≥1000 |
≥12 |
≥35 |
|
|
|
580°C age |
≥1000 |
≥865 |
≥13 |
≥31 |
|
|
|
620°C age |
≥930 |
≥325 |
≥16 |
≥28 |
|
|
|
HY 17-4PH Characteristic: |
|
|
|
|
|
||
|
High strength and hardness, good welding performance and corrosion resistance |
|||||||
|
|
|
|
|
|
|
|
|
|
HY 17-4PH Application range and field: |
|
|
|
|
|||
|
Used in components with high strength and corroson resistance |
|
||||||
| Regular shape for all kinds of alloys |
|||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Substantial Temp Nickel Centered & Tremendous Alloys – Mechanical Homes Inconel Round Bar, Plate Sheet Offer – Inconel is designed of Mostly Nickel and a number of other aspects. The origin coming from Supernovas. Inconel is a Tremendous Alloy and Michlin Metals sells Inconel Round Bar, Hex Bar, Flat Bar, Plate, Sheet, Tube and Pipe.
Melting down 1 gram bars of Silver, Copper, Nickel and Brass with hydrogen and oxygen. Brass is previously an alloy of copper and zinc, and did not soften down effortless as a I figured out from my Brass, Guide and Gunpowder video clip. I then blend the a few workable metals Silver, copper and nickel to generate…….Silvcopickel
SUBSCRIBE: http://comprehensive.sc/1bnslc9
Facebook: http://comprehensive.sc/1dT2aaM
RHNB Vs. Watermelon – http://comprehensive.sc/1bns60F
RHNB Vs. Jello – http://comprehensive.s/1bns0WF RHNB Vs. Elmers Glue – http://comprehensive.sc/1dT1TEM
RHNB Entire Playlist – http://comprehensive.sc/1dT1WjP -Want to ship an object / materials / substance to be RHNB’d or HHO’d? Send Here with a comprehensive credit of your donation! PO Box 21 96 Seymour St. Tonawanda NY 14150 Usa