30 Years Factory Iron Alloy Precision Alloy 1J50 Supply to America
Our eternal pursuits are the attitude of "regard the market, regard the custom, regard the science" and the theory of "quality the basic, trust the first and management the advanced" for 30 Years Factory Iron Alloy Precision Alloy 1J50 Supply to America, Standing still today and looking into the future, we sincerely welcome customers all over the world to cooperate with us.
HY J50 Material grades and equivalents
1J50 / JIS PB
HY J50 Chemical composition
|
Grade |
C |
P |
S |
Mn |
Ni |
Si |
Mn |
Cu |
Fe |
||||
|
≤ |
|||||||||||||
| HY J50 |
0.03 |
0.020 |
0.020 |
0.3-0.6 |
49.5-50.5 |
0.15-0.30 |
0.30-0.60 |
≤0.20 |
Rest |
||||
HY J50 Alloy Mechanical properties in the room temperature
|
Grade |
Shape |
Magnetic properties |
|||
|
Initial permeabilityμO |
Maximum permeabilityμm |
Hc |
Saturation induction density BS |
||
|
HY J50 |
Cold rolling strips |
≥3.8 |
≥62.5 |
≤9.6 |
1.5 |
|
Forging bar |
≥3.1 |
≥31.3 |
≤14.4 |
1.5 |
|
HY J50 Characteristic as below
The HY J50 has rectangular hysteresis loop and high saturation magnetic induction, is mainly used to worked at a moderate magnetic field magnetic amplifier, choke ring, rectifier circle, as well as the computer device components.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Qingdao NPA Marketplace Co. Ltd is a foremost manufacturer specialized in centrifugal casting tube and static castings of warmth resistant alloys, which include ethylene cracking furnace tube, reformer furnace tube, CAL(constant annealing traces) &CGL(constant galvanizing traces) furnace roller and radiant tube, glass lehr roller and warmth/have on resistant castings. The annual potential is 9000 tons centrifugal casting tube and 3500 tons static castings (500 tons precision castings).
Internet site: www.npa-china.com
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html