5 Years manufacturer Nickel cobalt base alloy AMS 5844 MP35N for Morocco Factory
Dedicated to strict quality control and thoughtful customer service, our experienced staff members are always available to discuss your requirements and ensure full customer satisfaction for 5 Years manufacturer Nickel cobalt base alloy AMS 5844 MP35N for Morocco Factory, If you are interested in any of our products and services, please don't hesitate to contact us. We are ready to reply you within 24 hours after receipt of your request and to create mutual un-limited benefits and business in near future.
HY MP35N Material grades and equivalents
MP35N/UNS R30035/ W.Nr 2.4999/ AMS 5844
Introduction:
HY MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties-ultra high strength, toughness, ductility and outstanding corrosion resistance. The alloy is work-strengthened and aged to obtain strength levels of 260 to 300 ksi(1793-2068 MPa). HY MP35N alloy resists corrosion in hydrogen sulfide, salt water and other chloride solution, as well as the mineral acids(nitric, hydrochloric, sulfuric).In addition, it has exceptional resistance to crevice and stress corrosion cracking in sea water and other hostile environments.
Chemical composition:
|
Weight% |
Ni |
Co |
Cr |
Mo |
Ti |
Fe |
Si |
Mn |
P |
B |
S |
C |
|
HY MP35N |
33 |
Balance |
19 |
9 |
1 |
1 |
0.15 |
0.15 |
0.015 |
0.01 |
0.01 |
0.03 |
|
37 |
21 |
10.5 |
Max |
Max |
Max |
Max |
Max |
Max |
Max |
Max |
Mechanical properties:
|
MP35N Alloy |
Ultimate Tensile |
0.2% Offset Yield |
Elongation in |
Reduction of Area |
Hardness |
Shear |
|
|
Typical Properties |
130 ksi(896 MPa) |
55 ksi(379 MPa) |
65% |
75% |
90 HRB |
— |
|
|
Typical Properties |
290 ksi(2000 MPa) |
280 ksi(1931 MPa) |
10% |
45% |
51 HRC |
— |
|
|
AMS 5844 Specification Requirements after Aging 4 Hours at 1000-1200℉ |
260 ksi(1795 MPa),min. |
230 ksi(1585 MPa),min. |
8%,min. |
35%,min. |
— |
150 ksi(1034 Mpa),min. |
|
The above data are longitudinal properties.
*Tensile properties will change depending on product size.
**Not required by AMS 5844, but this is guaranteed shear strength.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Turning insert brochures are obtainable for obtain at http://www.mitsubishicarbide.com/mmus/en/products/catalog/turning.html
Mitsubishi offers particular J-Series breakers and micro-grain grades for turning hard to minimize supplies. Mitsubishi breakers for warmth resistant alloys include the FJ (mild slicing), MJ (medium slicing) and GJ (medium to semi-weighty slicing). The presenting is concluded with the addition of the twin rake MS (medium slicing) breaker and spherical RCMX insert also for medium slicing. FJ and MJ collection insert are obtainable in G Class tolerances for applications that need a sturdy sharp slicing edge. For Titanium and non-ferrous supplies, the polished FJ-P/MJ-P edition is obtainable.
The FJ’s sharp slicing geometry is obtainable in common .002, .004, .008 and .016″ software nose radius. Although the MS and MJ software nose radius begins at .016 and the GJ at .031″ and up. Our warmth resistant alloy breakers are obtainable in a vast range of micro-grain grades particularly design for this market place phase. Our micro-grain grades are obtainable non-coated or topped off with PVD/CVD coatings and edge preparations to suit to the insert software range.
Out there uncoated grades are: RT9005, RT9010, TF15 and Hti10.
Our Miracle Coating (Al, Ti)N PVD grades are: VP05RT, VP10RT and VP15TF.
CVD coated US905 is design to deliver unequalled dress in resistance in stable higher velocity applications. The close microstructure of US905 CVD coatings limits insert flank and deal with dress in at higher speeds when in contrast to other merchandise. US905 has the best hardness cemented carbide substrate appropriate for CVD Coating.
To see all Mitsubishi Cutting Device products channels on YouTube, comply with url:
http://www.youtube.com/user/mitsubishicarbide/video clips?view=one
Or
Go to 1 of our products precise channels below:
The Cutting Edge: http://www.youtube.com/playlist?list=PL1CEA67C978F3029D&feature=view_all
Turning & Dull Channel: http://www.youtube.com/playlist?list=PL0D406ECCFFF53995&feature=view_all
Milling Channel: http://www.youtube.com/playlist?list=PL648BF1B051AE20F0&feature=view_all
Drilling Channel: http://www.youtube.com/playlist?list=PL6960075BD195101A&feature=view_all
Grooving Channel: http://www.youtube.com/playlist?list=PL3AD4CC3127719A38&feature=view_all
Swiss Tooling Channel: http://www.youtube.com/playlist?list=PL0FBAAF2F0230343C&feature=view_all
CBN Channel: http://www.youtube.com/playlist?list=PLBB88F97F9A2B5376&feature=view_all
Strong Carbide Close Mill Channel: http://www.youtube.com/playlist?list=PL7A1549BEF477EDDB&feature=view_all
Mitsubishi Elements Usa – Cutting Applications, Social Media Websites:
Fb: http://www.facebook.com/MitsubishiMaterials.US.CuttingTools
Twitter: http://twitter.com/#!/MMUSCuttingTool
YouTube: http://www.youtube.com/user/mitsubishicarbide
Supplemental Means:
Encounter Mitsubishi Carbide’s Patented On the internet Catalog with downloadable CAD information http://www.mitsubishicarbide.internet/mmus/en/catalogue/index.html
Extra Mitsubishi Cutting Device Films can be discovered at http://www.mitsubishicarbide.com/mmus/en/products/online video/index.html
Issues remember to speak to:
Complex Guidance at one-800-486-2341
Or
E mail MarketingServices@mmus.com
Protected specialized inquires can be submitted to Mitsubishi Elements at https://www.mitsubishicarbide.com/mailform/mmus/en/literature/sort.html
Thank you for using the time to view this online video and remember to take a look at Mitsubishi Elements Usa at http://www.mmus.com
This is our 4000 watt Co2 laser slicing process. We can cut Stainless Steel and alloys to .five hundred”, Steel and metal alloys to .750″ and aluminum to .375″. Equally our devices have big bed dimensions, just one is sixty” x 120″ and the 3000 watt is seventy eight” x 157″. Equally devices have automatic loading and shuttle tables for prototyping to manufacturing.