8 Years Manufacturer Nickel Alloy Inconel 625 UNS N06625 for Tunisia Factories
Our goal is to provide high quality products at competitive prices, and top-notch service to customers around the world. We are ISO9001, CE, and GS certified and strictly adhere to their quality specifications for 8 Years Manufacturer Nickel Alloy Inconel 625 UNS N06625 for Tunisia Factories, We fully welcome customers from all over the world to establish stable and mutually beneficial business relationships, to have a bright future together.
HY 625 Material grades and equivalents
Inconel 625/ GB NS336 / UNS N06625/ SEW VDIUV W.Nr.2.4856 NiCr22Mo9Nb / BS NA 12 / AFNOR NC22DNB
HY 625 Chemical composition
|
Alloy |
% |
Ni |
Cr |
Mo |
Nb+N |
Fe |
Al |
Ti |
C |
Mn |
Si |
Cu |
P |
S |
|
625 |
Min. |
58 |
20 |
8 |
3.15 |
|||||||||
|
Max. |
23 |
10 |
4.15 |
5 |
0.4 |
0.4 |
0.1 |
0.5 |
0.5 |
0.5 |
0.015 |
0.015 |
HY 625 Pysical properties
|
Density |
8.4 g/cm³ |
|
Melting point |
1290-1350°C |
HY 625 Alloy m inimum mechanical properties in the room temperature
|
Alloy state |
Tensile strength |
Yield strength |
Elongation A 5 % |
Brinell hardness |
|
625 |
760 |
345 |
30 |
≤220 |
Characteristic as below
1. Excellent corrosion resistance of different kinds of media in both oxidation and reduction environments.
2. Excellent resistance of pitting and crevice corrosion, and won’t happen stress corrosion cracking because of chloride.
3.Excellent resistance of the inorganic acid corrosion performance, such as nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid and the mixture of sulfuric acid and hydrochloric acid.
4. Excellent corrosion resistance of different kinds of inorganic acid mixture performance.
5. Good corrosion resistance of a variety of concentrations of hydrochloric acid when the temperature up to 40°C .
6. Good machining and welding, no weld cracking sensitivity.
7. Have pressure vessel authentication for the wall temperature between -196 ~ 450°C .
8. Apply for the highest standard lever VII of acidic environment by the NACE ( MR-01-75) authorized.
HY 625 Corrosion resistance
625 own a very good corrosion resistance in many media, especially with excellent resistance to pitting, crevice corrosion, intercrystalline corrosion, and erode in oxide, also good resistance to inorganic acid corrosion, such as nitric acid, phosphoric acid, sulfuric acid and hydrochloric acid. 625 can resist the alkali and organic acid corrosion in the oxidation and reduction environment. Effect resists the chloride reduction stress corrosion cracking. Normally no corrosion in the sea-water and industry environments since high corrosion resistance to the sea-water and salting liquid,as well as in high temperature, without sensitivity during welding. 625 have the resistance to oxidation and carbonizing in the static and cycle environments, also hacve the resistance the chlorine corrosion.
HY 625 Application field
Soften annealing low carbon alloy 625 widely used in the chemical process industry, good corrosion resistance and high strength made it an good choice for structural parts. 625 have application in sea-water for local mechanical stress attach.
HY 625 Typical application field as below
1 .The Organic chemical process parts contains chloride, especially in the use of acid chloride catalyst.
2. The digester and bleacherin the use of paper pulp and paper making industry.
3.Absorption tower, re-heater,gas import board, fan, blender, fair water fin, flue and so on for using in flue gas desulfurization system.
4. The equipment and parts in the use of acidic gas environments.
5. Acetic acid and anhydride reaction generator
6. Sulfur acid cooling
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Turning insert brochures are obtainable for obtain at http://www.mitsubishicarbide.com/mmus/en/products/catalog/turning.html
Mitsubishi offers particular J-Series breakers and micro-grain grades for turning hard to minimize supplies. Mitsubishi breakers for warmth resistant alloys include the FJ (mild slicing), MJ (medium slicing) and GJ (medium to semi-weighty slicing). The presenting is concluded with the addition of the twin rake MS (medium slicing) breaker and spherical RCMX insert also for medium slicing. FJ and MJ collection insert are obtainable in G Class tolerances for applications that need a sturdy sharp slicing edge. For Titanium and non-ferrous supplies, the polished FJ-P/MJ-P edition is obtainable.
The FJ’s sharp slicing geometry is obtainable in common .002, .004, .008 and .016″ software nose radius. Although the MS and MJ software nose radius begins at .016 and the GJ at .031″ and up. Our warmth resistant alloy breakers are obtainable in a vast range of micro-grain grades particularly design for this market place phase. Our micro-grain grades are obtainable non-coated or topped off with PVD/CVD coatings and edge preparations to suit to the insert software range.
Out there uncoated grades are: RT9005, RT9010, TF15 and Hti10.
Our Miracle Coating (Al, Ti)N PVD grades are: VP05RT, VP10RT and VP15TF.
CVD coated US905 is design to deliver unequalled dress in resistance in stable higher velocity applications. The close microstructure of US905 CVD coatings limits insert flank and deal with dress in at higher speeds when in contrast to other merchandise. US905 has the best hardness cemented carbide substrate appropriate for CVD Coating.
To see all Mitsubishi Cutting Device products channels on YouTube, comply with url:
http://www.youtube.com/user/mitsubishicarbide/video clips?view=one
Or
Go to 1 of our products precise channels below:
The Cutting Edge: http://www.youtube.com/playlist?list=PL1CEA67C978F3029D&feature=view_all
Turning & Dull Channel: http://www.youtube.com/playlist?list=PL0D406ECCFFF53995&feature=view_all
Milling Channel: http://www.youtube.com/playlist?list=PL648BF1B051AE20F0&feature=view_all
Drilling Channel: http://www.youtube.com/playlist?list=PL6960075BD195101A&feature=view_all
Grooving Channel: http://www.youtube.com/playlist?list=PL3AD4CC3127719A38&feature=view_all
Swiss Tooling Channel: http://www.youtube.com/playlist?list=PL0FBAAF2F0230343C&feature=view_all
CBN Channel: http://www.youtube.com/playlist?list=PLBB88F97F9A2B5376&feature=view_all
Strong Carbide Close Mill Channel: http://www.youtube.com/playlist?list=PL7A1549BEF477EDDB&feature=view_all
Mitsubishi Elements Usa – Cutting Applications, Social Media Websites:
Fb: http://www.facebook.com/MitsubishiMaterials.US.CuttingTools
Twitter: http://twitter.com/#!/MMUSCuttingTool
YouTube: http://www.youtube.com/user/mitsubishicarbide
Supplemental Means:
Encounter Mitsubishi Carbide’s Patented On the internet Catalog with downloadable CAD information http://www.mitsubishicarbide.internet/mmus/en/catalogue/index.html
Extra Mitsubishi Cutting Device Films can be discovered at http://www.mitsubishicarbide.com/mmus/en/products/online video/index.html
Issues remember to speak to:
Complex Guidance at one-800-486-2341
Or
E mail MarketingServices@mmus.com
Protected specialized inquires can be submitted to Mitsubishi Elements at https://www.mitsubishicarbide.com/mailform/mmus/en/literature/sort.html
Thank you for using the time to view this online video and remember to take a look at Mitsubishi Elements Usa at http://www.mmus.com
Substantial Temp Nickel Centered & Tremendous Alloys – Mechanical Homes Inconel Round Bar, Plate Sheet Offer – Inconel is designed of Mostly Nickel and a number of other aspects. The origin coming from Supernovas. Inconel is a Tremendous Alloy and Michlin Metals sells Inconel Round Bar, Hex Bar, Flat Bar, Plate, Sheet, Tube and Pipe.