Our team through professional training. Skilled professional knowledge, strong sense of service, to meet the service needs of customers for 80% OFF Price For Titanium alloy 6Al-2Sn-4Zr-2Mo UNS R54620 Export to Montpellier, If you are interested in any of our products and services, please don't hesitate to contact us. We are ready to reply you within 24 hours after receipt of your request and to create mutual un-limited benefits and business in near future.


HY Titanium 6-2-4-2 Material grades and equivalents

6Al-2Sn-4Zr-2Mo, 6-2-4-2 Titanium, 6-2-4-2, UNS R54620

Introduction

A near-alpha alloy, primarily used for high strength and toughness, with good creep resistance up to 1000°F. Forging and machining characteristics similar to those of Ti 6Al-4V. Applications include compressor components, hot airframe skin, and engine afterburner structures. The weld ability of Ti 6-2-4-2 is fair, using AMS 4952 weld wire. Several different treatments are available.

Chemistry Composition

 

Al

Sn

Zr

Mo

C

N

H

O

Si

Fe

Y

Others,
Each

Others,
Total

Ti

MIN

5.5

1.8

3.6

1.8

-

-

-

-

0.06

-

-

-

-

-

MAX

6.5

2.2

4.4

2.2

0.05

0.05

0.015

0.12

0.1

0.25

0.005

0.1

0.3

Balance

Features

  • Machinability similar to austenitic stainless steels
  • Easily welded if proper precautions are taken to prevent oxygen, nitrogen and hydrogen contaminations
  • Long term stability for temperatures up to 800°F

Applications

  • Compressor discs, blades
  • Airframe structure, skin
  • Engine afterburner components
  • Hush kits

Physical Properties

Density: 0.160 lb/in3

Beta Transus: 1825±25°F
Thermal Conductivity: 4.00 Btu • hr/ft2 • hr°F
Coefficient of Thermal Expansion: 32-212°F 4.3 x10-6 in/in°F
Modulus of Elasticity: 16.5×106 psi

Mechanical Properties

Minimum Tensile Properties, AMS 4919, Duplex Annealed

Thickness, in

0.025 ≤ 0.062

> 0.062 ≤ 1.000

> 1.000 ≤ 3.000

Tensile Strength, ksi

135,000

135,000

135,000

0.2% offset Yield Strength, ksi

125,000

125,000

125,000

Elongation, %

8

10

10

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !