We take "customer-friendly, quality-oriented, integrative, innovative" as objectives. "Truth and honesty" is our management ideal for Best Price for Iron Alloy Precision Alloy Invar 36 UNS K93600 for Naples Factories, If you are interested in our products, please feel free to send us your inquiry. We sincerely hope to establish win-win business relationships with you.
HY I36 Material grades and equivalents
GB 4J36/UNS K93600/AISI/ASTM Invar36/W.Nr.1.3912/Pernifer 36
Chemical composition
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Co |
Mo |
P |
S |
|
HY I36 |
Min. |
35 |
Balance |
||||||||
|
Max. |
38 |
0.5 |
0.1 |
0.06 |
0.35 |
1.0 |
0.5 |
0.02 |
0.025 |
Physical properties
|
Density |
8.1 g/cm3 |
|
Melting point |
1430 °C |
Mechanical properties in the room temperature
|
Alloy state |
Tensile strength Rm N/mm2 |
Yield strength RP0.2N/mm2 |
Elongation A5 % |
Brinell hardness HB |
|
HY I36 |
490 |
240 |
42 |
≤200 |
Characteristic
HY I36 alloy is a special ultra-low coefficient of heat expansion of low-iron-nickel alloy. One of carbon and manganese element of control is very important. Cold deformation can reduce the coefficient of thermal expansion, in particular within the framework of the heat treatment temperature coefficient of thermal expansion will enable stabilization. Has the following characteristics:
1.Has very low coefficient of heat expansion between the temperature of -250°C and 200°C.
2.Good toughness and plastic
Metallurgical structure
HY I36 is the face centered cubic lattice structure
Corrosion resistance
HY I36 has corrosion resistance in the dry air of room temperature. In other harsh environments, such as the humid air, there may be corrosion (rust).
Applied field
HY I36 suit for need to apply ultra-low coefficient of heat expansion environment. Typical applications are as follows:
1.Liquefied gas production, storage and transport
2.The measurement and control instruments work temperature lower than 200°C, such as temperature regulating device
3.Metals and other materials use the screw connector bush
4.Bimetal and bimetallic temperature controller
5.Film framework
6.Shadow mask
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen City GuangDong Province China
Substantial Temp Nickel Centered & Tremendous Alloys – Mechanical Homes Inconel Round Bar, Plate Sheet Offer – Inconel is designed of Mostly Nickel and a number of other aspects. The origin coming from Supernovas. Inconel is a Tremendous Alloy and Michlin Metals sells Inconel Round Bar, Hex Bar, Flat Bar, Plate, Sheet, Tube and Pipe.