Best Price for Nickel Alloy Incoloy 926 UNS N08926 for Latvia Factories
With our excellent management, strong technical capability and strict quality control system, we continue to provide our clients with reliable quality, reasonable prices and excellent services. We aim at becoming one of your most reliable partners and earning your satisfaction for Best Price for Nickel Alloy Incoloy 926 UNS N08926 for Latvia Factories, We welcome new and old customers from all walks of life to contact us for future business relationships and mutual success!
HY 926 Material grades and equivalents
Incoloy 926/ Alloy926/UNS N08926/W.Nr.1.4529
HY 926 Chemical composition:
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
Cu |
Mo |
N |
Ti |
P |
S |
|
926 |
Min. |
24 |
19 |
Balance |
0.5 |
6.0 |
0.15 |
0.6 |
|||||
|
Max. |
26 |
21 |
0.02 |
2 |
0.5 |
1.5 |
7.0 |
0.25 |
1.2 |
0.03 |
0.01 |
HY 926 Physical properties:
|
Density |
8.1 g/cm3 |
|
Melting point |
1320-1390 ℃ |
HY 926 Alloy Minimum Mechanical properties in the room temperature:
|
Alloy state |
Tensile strength |
Yield strength |
Elongation |
|
926 |
650 |
295 |
35 |
HY 926 Characteristic:
1.It has high resistance to pitting and crevice corrosion when in Halide and H2S contained acid media.
2.In practice, effective in resistance of chloride stress corrosion cracking.
3.A variety of corrosion have good corrosion resistance capability in the normal oxidation and restore environment.
4.Upgrade mechanical properties than Cronifer 1925 LC-Alloy 904 L.
5. Alloys has Improved the stability of metallurgical compared to a range of 18% of the nickel content alloys.
6.With a certification of applied in manufacturing-related pressure vessel (VdTUV-196~400℃ and ASME )
Metallurgical structure
926 is face-centered cubic lattice structure.
Corrosion resistance
926 is an austenitic stainless steel alloy has a similar chemical composition with 904L alloy, its nitrogen content is 0.2%, molybdenum content is 6.5%. Molybdenum and nitrogen content significantly increased the resistance of pitting and crevice corrosion in the halide media.Meantime, nickel and nitrogen not only ensures the stability of metallographical, but also reduce separating intergranular trend in the thermal process or welding process better than the nitrogen content of nickel alloy. 926 has particular corrosion resistance in the chloride ions medium due to the excellent local corrosion resistance and 25% nickel alloy content.A variety of experiments in the 10000-70000ppm of Chloride concentration, PH 5-6, 50-68℃ operating temperature of the slurry of limestone FGD system show that, after a 1-2 year trial period, 926 alloy without pitting and crevice corrosion.926 in other chemical media also has good corrosion resistance in the high temperature and high concentration of media, including sulfuric acid, phosphoric acid, acid gas, sea water, salt and organic acids.926 is the material that choosed for BAM directory Chapter 6 of “dangerous goods storage and transportation containers norms” by Berlin, Germany’s national Institute for Materials Research and Testing (BAM) . In addition, in order to have the best corrosion resistance only when the material is in the right state of metallurgy and guarantee clean conditions.
Application field:
Alloy 926 is a multipurpose material can be applied in many industrial:
1. Fire system, water purification system, marine engineering and hydraulic piping perfusion system
2. The pipeline, joint, air systems in the acidic gas production
3. Evaporator, the heat exchanger, filter, mixer, etc. in the phosphate production
4.Power plants condensation and pipe system in the use of sewage water to cool water
5. The use of acidic organic catalyst chlorinated derivatives production
6. The production of cellulose pulp bleacher
7. Polished bar in the orrosive oil wells
8. Hose system in the ocean engineering
9. Flue gas desulphurization system components
10. Sulfuric acid condensation and separation system
11. Crystalline salt concentration and the evaporator
12. Transport of corrosive chemicals containers
13. Reverse osmosis desalination plant
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Discovery and Science Channel’s How It truly is Designed Alloy Wheels episode.
All copyrights go to their respective homeowners.
Experimentální odlévání monelu na katedře strojírenské technologie při TU v Liberci – Monel je slitina niklu a mědi. Název Monel je registrován jako trademark americké firmy Specific Metals Corporation. Monel vyrobil v roce 1901 Robert Crooks Stanley, slitinu pojmenoval po tehdejším prezidentu firmy Ambrose Monellovi.
Monel vykazuje výborné mechanické vlastnosti a chemickou odolnost v náročném prostředí, např. v dlouhodobém kontaktu se slanou vodou, ale i v chemickém průmyslu. Často bývá využit tam, kde již nedostačují vlastnosti nerezových ocelí.
Monel is a group of nickel alloys, largely composed of nickel (up to sixty seven%) and copper, with tiny quantities of iron, manganese, carbon, and silicon. More powerful than pure nickel, Monel alloys are resistant to corrosion by quite a few agents, like promptly flowing seawater. They can be fabricated quickly by very hot- and chilly-working, machining, and welding.[2]
Monel was made by David H. Browne, main metallurgist for Global Nickel Co. Monel alloy four hundred is a binary alloy of the identical proportions of nickel and copper as is found naturally in the nickel ore from the Sudbury (Ontario) mines and is thus thought of a puritan alloy. Monel was named following business president Ambrose Monell, and patented in 1906.[three] Just one L was dropped, for the reason that loved ones names were being not allowed as trademarks at that time.[one] The title is now a trademark of Specific Metals Corporation.