Big Discount Heat Resistant Wire 0Cr25Al5 Fe-Cr-Al Alloy wire Wholesale to Poland

\

Short Introduction:


Product Detail

Product Tags

We insist on the principle of development of 'High quality, Efficiency, Sincerity and Down-to-earth working approach' to provide you with excellent service of processing for Big Discount Heat Resistant Wire 0Cr25Al5 Fe-Cr-Al Alloy wire Wholesale to Poland, Our company will continue to adhere to the " superior quality, reputable, the user first " principle wholeheartedly. We warmly welcome friends from all walks of life to visit and give guidance, work together and create a brilliant future!


HY 0255 Material grades and equivalents

0Cr25Al5 / 0Al5Cr25

HY 0255 Grade property performance

 Grade property performance

HY 0255

% Main Chemical Composition

Cr

23~26

Al

4.5~5.5

Fe

Balance

Mn

≤0.7

Nb

℃ Max contimnous service Temp. of element

1250

Resistivity mm2/m

1.42±0.07

10-5/℃ Temp coeff of resistance

5

g/cm3 Density 密度

7.1

Melting point≈ ℃ (approxi)

1500

Tensile strength N/mm2

637~784

% Elongation

>12

% Reducation of Area

65~75

Hardness(HB)

200~260

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy