Innovation, quality and reliability are the core values of our company. These principles today more than ever form the basis of our success as an internationally active mid-size company for Big Discount Nickel Alloy Inconel 783 UNS R30783 for South Korea Manufacturers, we are now looking forward to even greater cooperation with overseas customers based on mutual benefits. If you are interested in any of our products, please feel free to contact us for more details.


HY 783 Material grades and equivalents

Inconel 783 / Alloy 783 / UNS R30783

     An oxidation resistant low coefficient of thermal expansion (low CTE) superalloy developed for gas turbine applications.

The alloy is strengthened by a precipitation-hardening heat treatment made possible by additions of niobium and aluminum. In addition, the aluminum content provides excellent resistance to oxidation at high temperature.

The alloy’s density is 5% less than those of superalloys such as INCONEL alloy 718. The combination of low expansion, high strength and excellent resistance to oxidation makes the alloy especially useful for gas turbine and steam turbine components.

The low expansion enables closer control of clearances and tolerances for greater power output and fuel efficiency.

 

Table 1 - Limiting Chemical Composition*, %

Chromium……………………………………………………………. 2.5-3.5

Nickel ……………………………………………………………….26.0-30.0

Iron ……………………………………………………………………24.0-27.0

Niobium…………………………………………………………………2.5-3.5

Aluminum………………………………………………………………5.0-6.0

Cobalt………………………………………………………………Remainder

Boron……………………………………………………………..0.003-0.012

Carbon………………………………………………………………0.03 max.

Manganese………………………………………………………..0.50 max.

Silicon……………………………………………………………….0.50 max.

Phosphorus……………………………………………………..0.015 max.

Sulfur ……………………………………………………………….0.005 max

Titanium…………………………………………………………………0.1-0.4

Copper……………………………………………………………….0.50 max

 

Physical Properties

 

Table 2 - Physical Constants

Density, g/cm3…………………………………………………………..7.81

lb/in3………………………………………………………….0.282

Melting Range, °F ……………………………………………..2437-2565

°C …………………………………………….1336-1407

Specific Heat, Btu/lb•°F (77°F)……………………………………0.109

J/kg•°C (25°C)……………………………………….455

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy