Bottom price for Iron alloy Stainless Steel 17-4PH Export to Japan
We support our buyers with ideal high quality products and high level service. Becoming the specialist manufacturer in this sector, we have gained rich practical experience in producing and managing for Bottom price for Iron alloy Stainless Steel 17-4PH Export to Japan, "Create Values,Serving Customer!" is the aim we pursue. We sincerely hope that all customers will establish long term and mutually beneficial cooperation with us.If you wish to get more details about our company, Please contact with us now
|
HY 17-4PH Material grades and equivalents |
|
||
|
UNS |
AISI/ASTM |
JIS |
W.Nr |
|
S17400 |
630,17-4PH |
SUS630 |
1.4542 |
|
HY 17-4PH Chemical composition: |
|
|
|
|
|
|
|
|
|||
|
Alloy |
% |
Ni |
Cr |
Fe |
C |
Mn |
Si |
S |
Cu |
Nb |
P |
|
HY 17-4PH |
Min. |
3 |
15.5 |
balance |
|
|
|
|
3 |
0.15 |
|
|
Max. |
5 |
17.5 |
0.07 |
1 |
1 |
0.03 |
5 |
0.45 |
0.035 |
||
|
HY 17-4PH Physical properties |
||
|
Density |
7.78/cm3 |
|
|
Melting point |
1400-1440 °C |
|
|
HY 17-4PH Minimum mechanical properties in the room temperature |
||||||
|
Status |
Tensile strength |
Yield strength |
Elongation |
HRC(HBS) |
|
|
|
Rm N/mm² |
Rp0.2 N/mm² |
A5 % |
|
|
||
|
480°C age |
≥1310 |
≥1180 |
≥10 |
≥40 |
|
|
|
550°C Age |
≥1060 |
≥1000 |
≥12 |
≥35 |
|
|
|
580°C age |
≥1000 |
≥865 |
≥13 |
≥31 |
|
|
|
620°C age |
≥930 |
≥325 |
≥16 |
≥28 |
|
|
|
HY 17-4PH Characteristic: |
|
|
|
|
|
||
|
High strength and hardness, good welding performance and corrosion resistance |
|||||||
|
|
|
|
|
|
|
|
|
|
HY 17-4PH Application range and field: |
|
|
|
|
|||
|
Used in components with high strength and corroson resistance |
|
||||||
| Regular shape for all kinds of alloys |
|||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen City GuangDong Province China
Riporto(placcatura)con filo Nimonic 80 dia. one.2 eseguito con inverter multiprocesso Weldtronic Synertech 8004 Digit in pulsato sinergico.
NB .Il lampeggio dell’arco è presente solo nella ripresa effettuata dalla fotocamera digitale usata probabilmente a causa di interferenza con l’intenso arco luminoso.
Details: belda1@tiscali.it