Bottom price for Nickel cobalt base alloy AMS 5844 MP35N for Thailand Factories
We always think and practice corresponding to the change of circumstance, and grow up. We aim at the achievement of a richer mind and body and the living for Bottom price for Nickel cobalt base alloy AMS 5844 MP35N for Thailand Factories, Standing still today and looking into the future, we sincerely welcome customers all over the world to cooperate with us.
HY MP35N Material grades and equivalents
MP35N/UNS R30035/ W.Nr 2.4999/ AMS 5844
Introduction:
HY MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties-ultra high strength, toughness, ductility and outstanding corrosion resistance. The alloy is work-strengthened and aged to obtain strength levels of 260 to 300 ksi(1793-2068 MPa). HY MP35N alloy resists corrosion in hydrogen sulfide, salt water and other chloride solution, as well as the mineral acids(nitric, hydrochloric, sulfuric).In addition, it has exceptional resistance to crevice and stress corrosion cracking in sea water and other hostile environments.
Chemical composition:
|
Weight% |
Ni |
Co |
Cr |
Mo |
Ti |
Fe |
Si |
Mn |
P |
B |
S |
C |
|
HY MP35N |
33 |
Balance |
19 |
9 |
1 |
1 |
0.15 |
0.15 |
0.015 |
0.01 |
0.01 |
0.03 |
|
37 |
21 |
10.5 |
Max |
Max |
Max |
Max |
Max |
Max |
Max |
Max |
Mechanical properties:
|
MP35N Alloy |
Ultimate Tensile |
0.2% Offset Yield |
Elongation in |
Reduction of Area |
Hardness |
Shear |
|
|
Typical Properties |
130 ksi(896 MPa) |
55 ksi(379 MPa) |
65% |
75% |
90 HRB |
— |
|
|
Typical Properties |
290 ksi(2000 MPa) |
280 ksi(1931 MPa) |
10% |
45% |
51 HRC |
— |
|
|
AMS 5844 Specification Requirements after Aging 4 Hours at 1000-1200℉ |
260 ksi(1795 MPa),min. |
230 ksi(1585 MPa),min. |
8%,min. |
35%,min. |
— |
150 ksi(1034 Mpa),min. |
|
The above data are longitudinal properties.
*Tensile properties will change depending on product size.
**Not required by AMS 5844, but this is guaranteed shear strength.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Movie da parte di Costanzo Perico
Experimentální odlévání monelu na katedře strojírenské technologie při TU v Liberci – Monel je slitina niklu a mědi. Název Monel je registrován jako trademark americké firmy Specific Metals Corporation. Monel vyrobil v roce 1901 Robert Crooks Stanley, slitinu pojmenoval po tehdejším prezidentu firmy Ambrose Monellovi.
Monel vykazuje výborné mechanické vlastnosti a chemickou odolnost v náročném prostředí, např. v dlouhodobém kontaktu se slanou vodou, ale i v chemickém průmyslu. Často bývá využit tam, kde již nedostačují vlastnosti nerezových ocelí.
Monel is a group of nickel alloys, largely composed of nickel (up to sixty seven%) and copper, with tiny quantities of iron, manganese, carbon, and silicon. More powerful than pure nickel, Monel alloys are resistant to corrosion by quite a few agents, like promptly flowing seawater. They can be fabricated quickly by very hot- and chilly-working, machining, and welding.[2]
Monel was made by David H. Browne, main metallurgist for Global Nickel Co. Monel alloy four hundred is a binary alloy of the identical proportions of nickel and copper as is found naturally in the nickel ore from the Sudbury (Ontario) mines and is thus thought of a puritan alloy. Monel was named following business president Ambrose Monell, and patented in 1906.[three] Just one L was dropped, for the reason that loved ones names were being not allowed as trademarks at that time.[one] The title is now a trademark of Specific Metals Corporation.