Dedicated to strict quality control and thoughtful customer service, our experienced staff members are always available to discuss your requirements and ensure full customer satisfaction for Cheap PriceList for Nickel Alloy Inconel 600 UNS N06600 Factory from Moldova, Looking to the future, a long way to go, constantly striving to become the all staff with full enthusiasm, one hundred times the confidence and put our company built a beautiful environment, advanced products, quality first-class modern enterprise and work hard!


HY 600 Material grades and equivalents

HY 600 Inconel 600/ GB NS312 / UNS N06600 / SEW VDIUV W.Nr.2.4816 NiCrl 5Fe/ BS NA14 / AFNOR NC15FE

HY 600 Chemical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Cu

P

S

600

Min.

72

14

6

Max.

17

10

0.15

1

0.5

0.5

0.015

0.015

HY 600 Physical properties:

Density

8.4 g/cm3

Melting Point

1370-1425 ℃

HY 600 Alloy m inimum Mechanical properties in the room temperature:

Aolly status

Tensile strength

Yield strength

Elongation

Brinell hardness

Rm N/mm2

R P 0. 2N/mm2

A 5 %

HB

Annealing treatment

550

240

30

≤195

Solution treatment

500

180

35

≤185

HY 600 Characteristic as below:
1.Good corrosion resistance property for the reduction, oxidation, Nitric and other media. 2.Good stress corrosion cracking resistance property in both room temperature and high temperature.
3.Good corrosion resistance of the dry chlorine and chlorine hydride.
4.Good mechanical property when below zero, room temperature and high temperature.
5.Good anti-creep rupture strength, with the recommendation of 700℃ or above working environment.

HY 600 Metallurgical structure
600 is face-centered cubic lattice structure.

HY 600 Corrosion resistance
600 have corrosion resistance to many kinds of corrosive media. Chromium content made it with better corrosion resistance than Nickel 99.2 (alloy200) and Nickel 99.2 ( alloy201,low carbon) in the oxidize environment. Meantime, high Nickel content make this alloy with good corrosion resistance in the reduction condition and alkaline solution, and also effective avoid chlorine-iron stress corrosion cracking. 600 have good corrosion resistance in the acid, acetic acid, formic acid, stearic acid and other organic acid, with medium corrosion resistance in the inorganic acid. The alloy with excellent corrosion resistance in the first and the second recycling use of the high purity water in the nuclear reactor. Especially excellent corrosion resistance to dry chlorine and chlorine hydride applied up to 650 ℃. When nder the high temperature, annealing and state solution alloy have good antioxidant off and high-intensity in the air, 600 can resist the ammonia, nitriding and carburizing atmosphere, but at the turn of the changes in redox conditions, it will be corrosion by parts of oxidation media.( such as green death liquid)

HY 600 Application field:
1. Erosion thermocouple sheath of the atmosphere
2.Vinyl chloride monomer production: corrosion resistance to chlorine, hydrogen chloride, oxidation and carbonation.
3. Oxide shaft chloride converted to six fluoride: hydrogen fluoride anti-corrosion.
4. Corrosive alkali metal produce and usage filed, especially the sulfide use environment.
5. Use Chlorine produce titanium dioxide
6.Organic or inorganic chlorine produce: corrosion resistance to chlorine and fluoride.
7. Nuclear reactor
8.Heat treatment furnace flask and components, especially in the carbonization and nitride atmosphere.
9. Petrochemical works production of catalytic regeneration in the application of more than 700℃ recommended the use of 600, in order to obtain a longer service life.

Regular shape for all kinds of alloys
Form Specification Supply Form Others
Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E
Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D
Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E
Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling
Forged barΦ26-245mm,Length≤4000mm
Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement
Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement
Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy
Flangs All kinds of Flangs Base on your requirement Steel, Alloy
Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France.
Straight WireΦ1.6mm-4.0mm
Welding rodΦ1.2mm-4.0mm
Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy
Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy

  • Previous:
  • Next:

  • RELATED PRODUCTS

    WhatsApp Online Chat !