Cheapest Price Heat Resistant Wire 0Cr21Al6Nb Fe-Cr-Al Alloy wire to New Delhi Importers
We believe in: Innovation is our soul and spirit. Quality is our life. Customer need is our God for Cheapest Price Heat Resistant Wire 0Cr21Al6Nb Fe-Cr-Al Alloy wire to New Delhi Importers, "Create Values,Serving Customer!" is the aim we pursue. We sincerely hope that all customers will establish long term and mutually beneficial cooperation with us.If you wish to get more details about our company, Please contact with us now
HY 0216Nb Material grades and equivalents
0Cr21Al6Nb / 0Al6NbCr21
HY 0216Nb Grade property performance
|
Grade property performance |
HY 0216Nb |
|
|
% Main Chemical Composition |
Cr |
21~23 |
|
Al |
5~7 |
|
|
Fe |
Balance |
|
|
Mn |
≤0.7 |
|
|
Nb |
0.5 |
|
|
℃ Max contimnous service Temp. of element |
1350 |
|
|
Resistivity mm2/m |
1.45±0.07 |
|
|
10-5/℃ Temp coeff of resistance |
5 |
|
|
g/cm3 Density |
7.1 |
|
|
Melting point≈ ℃ (approxi) |
1510 |
|
|
Tensile strength N/mm2 |
637~784 |
|
|
% Elongation |
>12 |
|
|
% Reducation of Area |
65~75 |
|
|
Hardness(HB) |
200~260 |
|
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
http://www.weldingtipsandtricks.com/metals-and-how-to-weld-nickel.html
How to weld nickel alloys like hastelloy, inconel, etc. Nickel alloys have a low thermal conductivity and so limiting heat input and using lower amperage than would be used for stainless is one key to making good nickel alloy welds.
Inconel 718, The Severe Metal Alloy. http://www.techsteel.web/alloy/nickel/inconel-718
Turbine Blades have revolutionized air vacation and electricity era.
Hundreds of slim precision blades spinning at a hundred,000 RPM have to have a materials that can stand up to excessive disorders.
Inconel 718 is a distinctive metal alloy that can stand up to excessive temperatures from -423° to 1300°F
This alloy is aged hardened, making it possible for it to be welded without having hardening for the duration of heating and cooling.
The improvement of Inconel began in the fifties for use in vital steam line plants. Originally used for armed service programs it was later on adopted by the professional sector.
Inconel 718‘s tolerance for excessive temperature make it specially perfectly suited for programs such as
turbine blades
nuclear electricity plants, and
aerospace programs. It was used in the space shuttles high force pump.
AMS 5589 | AMS 5596 | AMS 5597 | AMS 5663 | AMS 5664
For extra inconel 718 details take a look at techsteel.web
Tech Steel provides Specialty Alloys and Supplies.
Check out www.techsteel.web or phone 1-631-223-7638