Our team through professional training. Skilled professional knowledge, strong sense of service, to meet the service needs of customers for China Cheap price Heat Resistant Wire 0Cr21Al6Nb Fe-Cr-Al Alloy wire for Ecuador Importers, Create Values,Serving Customer!" is the aim we pursue. We sincerely hope that all customers will establish long term and mutually beneficial cooperation with us.If you wish to get more details about our company, Please contact with us now.
HY 0216Nb Material grades and equivalents
0Cr21Al6Nb / 0Al6NbCr21
HY 0216Nb Grade property performance
|
Grade property performance |
HY 0216Nb |
|
|
% Main Chemical Composition |
Cr |
21~23 |
|
Al |
5~7 |
|
|
Fe |
Balance |
|
|
Mn |
≤0.7 |
|
|
Nb |
0.5 |
|
|
℃ Max contimnous service Temp. of element |
1350 |
|
|
Resistivity mm2/m |
1.45±0.07 |
|
|
10-5/℃ Temp coeff of resistance |
5 |
|
|
g/cm3 Density |
7.1 |
|
|
Melting point≈ ℃ (approxi) |
1510 |
|
|
Tensile strength N/mm2 |
637~784 |
|
|
% Elongation |
>12 |
|
|
% Reducation of Area |
65~75 |
|
|
Hardness(HB) |
200~260 |
|
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |