China Manufacturer for Heat Resistant Wire 0Cr21Al4 Fe-Cr-Al Alloy wire Factory from Barbados
To constantly improve the management system by virtue of the rule of "sincerely, good faith and quality are the base of enterprise development", we widely absorb the essence of related products internationally, and constantly develop new products to meet the demands of customers for China Manufacturer for Heat Resistant Wire 0Cr21Al4 Fe-Cr-Al Alloy wire Factory from Barbados, We welcome new and old customers from all walks of life to contact us for future business relationships and mutual success.
HY 0214 Material grades and equivalents
0Cr21Al4 / 0Al4Cr21
HY 0214Grade property performance
|
Grade property performance |
HY 0214 |
|
|
% Main Chemical Composition |
Cr |
17~21 |
|
Al |
2~4 |
|
|
Fe |
Balance |
|
|
Mn |
≤0.7 |
|
|
Nb |
— |
|
|
℃ Max contimnous service Temp. of element |
1100 |
|
|
Resistivity mm2/m |
1.23±0.06 |
|
|
10-5/℃ Temp coeff of resistance |
5 |
|
|
g/cm3 Density |
7.35 |
|
|
Melting point≈ ℃ (approxi) |
1500 |
|
|
Tensile strength N/mm2 |
637~784 |
|
|
% Elongation |
>14 |
|
|
% Reducation of Area |
65~75 |
|
|
Hardness(HB) |
200~260 |
|
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
Supplier foil、strip、sheet、coil、plate、wire、rod、bar、tube、pipe、flat ribbon、Profiled wire…
BuildingNo.1,Third Industrial District XiTou Village SongGang Town Bao’An District ShenZhen City GuangDong Province China
Discovery and Science Channel’s How It truly is Designed Alloy Wheels episode.
All copyrights go to their respective homeowners.