China Manufacturer for Nickel Alloy Monel K500 UNS N05500 for Jakarta Factories
We insist on offering high quality production with good business concept, honest sales and the best and fast service. it will bring you not only the high quality product and huge profit, but the most significant is to occupy the endless market for China Manufacturer for Nickel Alloy Monel K500 UNS N05500 for Jakarta Factories, We are confident to make great achievements in the future. We are looking forward to becoming one of your most reliable suppliers.
HY MK-500 Material grades and equivalents
Monel K-500/W Nr.2.4375/Nickel-Copper Alloy 500/UNS N05500
HY MK-500 Chemical composition:
| Alloy |
% |
Ni |
Cu |
Al |
Ti |
Fe |
Mn |
S |
C |
Si |
|
Monle K500 |
Min. |
63 |
27.0 |
2.30 |
0.35 |
|||||
|
Max. |
33.0 |
3.15 |
0.85 |
2.0 |
1.5 |
0.01 |
0.25 |
0.5 |
HY MK-500 Physical properties:
|
Density |
8.44 g/cm3 |
|
Melting point |
1315-1350℃ |
HY MK-500 minimum mechanical properties in the room temperature:
| Forms | Condition | Max. section Thickness,in.(mm) | Tensile strength Min. Ksi.(Mpa) | Yield strength Min.Ksi.(Mpa) | Elongation in 2 in,or 4D,min.,% | Hardness | |
| HB min. | HRC min. | ||||||
| Round bars, Hexagons, squares, rectangles and forgings | hot-worked and age hardened | All Sizes | 140(965) | 100(690) | 20 | 265 | 27 |
| Round bars | cold worked and age hardened | 1/4(6.4)to 1(25.4) | 145(1000) | 110(760) | 15 | 300 | 32 |
| over 1(25.4)to 3(76.2) | 140(965) | 100(690) | 17 | 280 | 29 | ||
| over 3(76.2)to 4(101.6) | 135(930) | 99(655) | 20 | 255 | 25 | ||
| Hexagons | cold worked and age hardened | 1/4(6.4)to 2(50.8) | 140(965) | 100(690) | 15 | 265 | 27 |
| Round bars, Hexagons, squares, rectangles and forgings | Annealed and age hardened | Up to 1(25.4) | 130(895) | 90(620) | 20 | 250 | 24 |
| 1(25.4)and over | 130(895) | 85(585) | 20 | 250 | 24 | ||
HY MK-500 has approximately twice the tensile strength and triple the yield strength of Alloy 400. The strength of Alloy K-500 is maintained to 1200 degrees Fahrenheit, but stays ductile and tough down to temperatures of -400 degrees Fahrenheit. Alloy K-500 also stays non-magnetic to -200 degrees Fahrenheit.
Additional characteristics of Alloy K-500 include outstanding corrosion resistance in a wide range of chemical and marine surroundings, from salts and alkalis, non-oxidizing acids to pure water. HY MK-500 is non-magnetic and spark resistant. It is also recommended that Alloy K-500 be annealed when it is welded and that any weldments be stress relieved prior to aging.
Industries Served:
- gas & oil extraction
- chemical processing
- marine engineering
Regular shape for all kinds of alloys Form Specification Supply Form Others Sheet Thickness:0.40-4.75mm,General Width:1000、1219、1500mm Whole Coil or piece of it Cold Annealed,Surface 2B、2E Plate Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) Whole Coil or piece of it Single hot rolling,Solid solution annealed state,Surface 1D Belt Thickness:0.10-3.0mm,Width:50-500mm Whole Coil or Specified size Cold Annealed,Surface 2B、2E Bar & Rod Rolled barΦ5-45mm,Length≤1500mm Polished Bar(circle、Square) Solution annealing,descaling Forged barΦ26-245mm,Length≤4000mm Weld tube Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm Base on your requirement Seamless Tube Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm Base on your requirement Wire Outer diameterΦ0.1-13mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy Forged piece discs,rings,squares,blocks,slabs Base on your requirement Steel, Alloy Flangs All kinds of Flangs Base on your requirement Steel, Alloy Welding Material Coil wire Φ0.025mm-1.6mm Base on your requirement Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. Straight WireΦ1.6mm-4.0mm Welding rodΦ1.2mm-4.0mm Tube Elbow, three links, four links, different diameter size Base on your requirement Ni & Ni alloy, Ti & Ti alloy Explosive bonded laminate Raw Sheet Thickness≥2mm Base on your requirement Ni & Ni alloy, Ti & Ti alloy
A nitinol wire/form memory alloy inchworm that walks across a table employing only warmth. The warmth is supplied by electrical existing heating up the skinny nitinol wire, causing it to return to its remembered form, a compressed coil in this scenario. A V-formed spring returns it to the commencing form.
Guidance RimstarOrg on Patreon https://www.patreon.com/user?u=680159
Subscribe for new films every single week http://www.youtube.com/user/rimstarorg?sub_affirmation=1
Go to the principal channel webpage below https://youtube.com/rimstarorg
See also:
How to Make Nitinol Wire Inchworm (Shape Memory Alloy)
https://www.youtube.com/look at?v=getfzfZJjHM
Nitinol Wire – How to Use it
https://www.youtube.com/look at?v=4Yi4epJ83EE
How a Rocket Performs/Earth to Area Eg SpaceX Falcon 9 and Dragon
https://www.youtube.com/look at?v=L0AMQ6kRNMA
My webpage about this nitinol wire inchworm:
http://rimstar.org/science_electronics_tasks/nitinol_wire_inchworm_form_memory_alloy_handmade.htm
Adhere to at the rear of-the-scenes on:
Twitter https://twitter.com/#!/RimStarz
Google+ https://additionally.google.com/116395125136223897621
Fb https://www.fb.com/rimstarorg
http://rimstar.org
The inspiration came from this one:
https://www.youtube.com/look at?v=DW4WaTmoZ3c
Essence – audio by audionautix.com
Melting down 1 gram bars of Silver, Copper, Nickel and Brass with hydrogen and oxygen. Brass is previously an alloy of copper and zinc, and did not soften down effortless as a I figured out from my Brass, Guide and Gunpowder video clip. I then blend the a few workable metals Silver, copper and nickel to generate…….Silvcopickel
SUBSCRIBE: http://comprehensive.sc/1bnslc9
Facebook: http://comprehensive.sc/1dT2aaM
RHNB Vs. Watermelon – http://comprehensive.sc/1bns60F
RHNB Vs. Jello – http://comprehensive.s/1bns0WF RHNB Vs. Elmers Glue – http://comprehensive.sc/1dT1TEM
RHNB Entire Playlist – http://comprehensive.sc/1dT1WjP -Want to ship an object / materials / substance to be RHNB’d or HHO’d? Send Here with a comprehensive credit of your donation! PO Box 21 96 Seymour St. Tonawanda NY 14150 Usa