China Top 10 Iron Alloy Precision Alloy 4J29 F15 Manufacturer in luzern
abide by the contract", conforms to the market requirement, joins in the market competition by its high quality as well as provides more comprehensive and excellent service for clients to let them become big winner. The pursue of the company, is the clients' satisfaction for China Top 10 Iron Alloy Precision Alloy 4J29 F15 Manufacturer in luzern, Contact with us today! We are ready for the market service now!
HY J29 Material grades and equivalents
4J29/AISI/ASTM F15/JIS EMAS-1001/W.Nr 1.3912
HY J29 Chemical composition
|
Alloy |
% |
Ni |
Cr |
Fe |
Co |
Cu |
C |
Mn |
Si |
P |
S |
Mo |
|
HY J29 |
Min |
28.5 |
Rest |
16.8 |
||||||||
|
Max |
29.5 |
0.2 |
17.8 |
0.20 |
0.03 |
0.50 |
0.30 |
0.02 |
0.02 |
0.20 |
HY J29 Alloy Mechanical properties in the room temperature
|
Grade |
Average linear expansion factor(10-6℃) |
||||||
|
20℃~100℃ |
20℃~300℃ |
20℃~400℃ |
20℃~450℃ |
20℃~500℃ |
20℃~530℃ |
20℃~600℃ |
|
|
HY J29 |
- |
- |
4.6~5.2 |
5.1~5.5 |
- |
- |
- |
HY J29 Characteristic as below
HY J29 having similar coefficient of linear expansion with hard glass within a certain temperature range, applied to vacuum industry to match hard glass.
| Regular shape for all kinds of alloys | |||
| Form | Specification | Supply Form | Others |
| Sheet | Thickness:0.40-4.75mm,General Width:1000、1219、1500mm | Whole Coil or piece of it | Cold Annealed,Surface 2B、2E |
| Plate | Thickness:4.76-60mm,Width:1500、2000、2500mm,Length:3000、6000、8000、8500mm(Under 10mm plate can be coiled) | Whole Coil or piece of it | Single hot rolling,Solid solution annealed state,Surface 1D |
| Belt | Thickness:0.10-3.0mm,Width:50-500mm | Whole Coil or Specified size | Cold Annealed,Surface 2B、2E |
| Bar & Rod | Rolled barΦ5-45mm,Length≤1500mm | Polished Bar(circle、Square) | Solution annealing,descaling |
| Forged barΦ26-245mm,Length≤4000mm | |||
| Weld tube | Outer diameterΦ4.76-135mm,Wall Thickness0.25-4.00mm,Length:≤35000 mm | Base on your requirement | |
| Seamless Tube | Outer diameterΦ3-114mm,Wall Thickness0.2-4.5mm | Base on your requirement | |
| Wire | Outer diameterΦ0.1-13mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Forged piece | discs,rings,squares,blocks,slabs | Base on your requirement | Steel, Alloy |
| Flangs | All kinds of Flangs | Base on your requirement | Steel, Alloy |
| Welding Material | Coil wire Φ0.025mm-1.6mm | Base on your requirement | Certificate of Origin:America, Sweden, Britain, Germany, Austria, Italy, France. |
| Straight WireΦ1.6mm-4.0mm | |||
| Welding rodΦ1.2mm-4.0mm | |||
| Tube | Elbow, three links, four links, different diameter size | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
| Explosive bonded laminate | Raw Sheet Thickness≥2mm | Base on your requirement | Ni & Ni alloy, Ti & Ti alloy |
The progress of improved metallic resources is a crucial action at the leading edge of science and know-how. Metals offer unrivalled mixtures of houses and reliability at a cost which is economical. They are adaptable mainly because subtle improvements in their microstructure can cause dramatic variations in their houses. For illustration, it is feasible to purchase business steel with a energy as lower as 50 MPa or as large as 5500 MPa. They can be built with a microstructure which is finer than that of carbon nanotubes. An understanding of the progress of microstructure in metals, rooted in thermodynamics, crystallography and kinetic phenomena is crucial for the resources scientist. The bulk of the 1.4 billion tonnes of metals made annually are the outcome of developments within just the last 10 a long time
http://www.msm.cam.ac.british isles/phase-trans/2002/creep.1.html
.025″ slash, 140sfm, VBMT 331 insert